Buyers Guide Home PageAdd a Hot Link

GMAW Power Source Buyers' Guide©

Model
or
Series
Type of
Power
Source
Wire Feed
Options
Wire Feed
Speed
Range
Running Gear Std. Applicable Processes Output Rating (DC) Input Rating
GTAW GMAW SMAW FCAW GMAWP GTAWP Carbon Arc Brazing Spot CACA SAW Other Gouging Amps Voltage Duty Cycle Volts Phase Hz

 ESAB WELDING & CUTTING PRODUCTS Florence, SC   Hot Link

Migmaster 253
Transformer rectifier
Built-in
74 - 748
checkbox   checkbox   checkbox       checkbox checkbox         
250
23
20
208/230
1
50/60
Migmaster 250
Transformer rectifier
Built-in
20 - 650
checkbox   checkbox checkbox         checkbox checkbox         
250
27
50
208/230/380/400/460/575
1
50/60
Multimaster 160
Inverter multiprocess CV & CC
Built-in
65 - 650
  checkbox checkbox checkbox checkbox       checkbox           
160
23
60
208/230
1
50/60
Multimaster 260
Switch mode multiprocess
Built-in
65 - 675
checkbox checkbox checkbox checkbox checkbox checkbox     checkbox checkbox         
260
27
50
208/230/460/575
1
50/60
353cv
Transformer rectifier
External
      checkbox   checkbox       checkbox           
350
34
100
230/400/460/575
3
50/60
453cv
Transformer rectifier
External
      checkbox   checkbox     checkbox checkbox    checkbox checkbox   checkbox
450
38
100
230/400/460/575
3
50/60
653cvcc
Transformer rectifier multiprocess CV & CC
External
    checkbox checkbox checkbox checkbox     checkbox checkbox    checkbox checkbox   checkbox
650
44
100
230/400/460/575
3
50/60
MultiPower 460
Switch mode multiprocess CV & CC
External
    checkbox checkbox checkbox checkbox checkbox   checkbox checkbox    checkbox checkbox   checkbox
450
38
100
230/460/575
3
50/60
SVI-450i
Inverter multiprocess CV & CC
External
    checkbox checkbox checkbox checkbox checkbox     checkbox    checkbox      
450
38
60
208/220/380/415/460
1/3
50/60
Aristo 500
Microbased inverter multiprocess CV & CC
External dedicated
    checkbox checkbox checkbox checkbox checkbox checkbox checkbox checkbox    checkbox     checkbox
500
39
60
460
3
50/60

 HTP AMERICA INC. Arlington Heights, IL   Hot Link

HTP Mig 200
Transformer Rectifier
Spool Gun
7 - 625
checkbox   checkbox   checkbox       checkbox checkbox         
200
20 - 37 OCV
20@200A 100@105A
208/240
1
50/60
MTS 160
Inverter
Spool Gun
60 - 500
  checkbox checkbox checkbox checkbox       checkbox           
150
20 - 25 OCV
40@150A
220
1
50/60
HTP Mig 140
Transformer Rectifier
Spool Gun
7 - 475
checkbox   checkbox checkbox         checkbox checkbox         
140
20 - 35 OCV
20@140A 100@62A
115
1
50/60
HTP Mig 160
Transformer Rectifier
Spool Gun
7 - 625
checkbox   checkbox   checkbox       checkbox checkbox         
160
19 - 35 OCV
20@160A 100@78A
208/240
1
50/60
HTP Mig 160DV
Transformer Rectifier
Spool Gun
7 - 625
checkbox   checkbox checkbox         checkbox checkbox         
160
17 - 35 OCV
20@160A 100@78A
110/220
1
50/60
HTP Mig 2400
Transformer Rectifier
Spool Gun
7 - 625
checkbox   checkbox   checkbox       checkbox checkbox         
240
18 - 38 OCV
35@240A 100@142A
208/240
1
50/60

 OTC DAIHEN INC. Tipp City, OH   Hot Link

DM350
Digital Inverter
External
  checkbox   checkbox   checkbox       checkbox checkbox         
30 - 350
31.5
60@350A
208/230/460
1/3
50/60
DP400
Digital Inverter
External
  checkbox   checkbox   checkbox checkbox     checkbox checkbox         
30 - 400
34
50@400A
208/230/460
3
50/60
DP500
Digital Inverter
External
  checkbox   checkbox   checkbox checkbox     checkbox checkbox         
30 - 500
39
100@350A / 60@500A
460
3
50/60
DL350
Digital Inverter
External
  checkbox   checkbox                       
350
36
60
208
3
50/60
DW300
Digital Inverter
External
  checkbox   checkbox   checkbox checkbox     checkbox           
300
29
80
29
3
50/60

 ASTRO ARC POLYSOUDE Valencia, CA

PC STT MIG-MAG
Inverter
Polyfil
300
    checkbox     checkbox                             
PC MIG-MAG 405
Inverter
Polyfil
300
    checkbox     checkbox                             
PC MIG-MAG Combined STT 455
Inverter
Polyfil
300
    checkbox     checkbox                             

 FRONIUS USA LLC Brighton, MI

Vario Star 1500
Transformer
Built -n
39 - 709
checkbox   checkbox   checkbox       checkbox checkbox         
3 - 140
15 - 21
60@85A
230
1
50/60
Vario Star 2500
Transformer
Built-in
39 - 709
checkbox   checkbox   checkbox       checkbox checkbox         
3 - 250
15.3 - 26.5
60@185A
230/460
3
50/60
Vario Star 3100
Transformer
Built-in
39 - 709
checkbox   checkbox   checkbox       checkbox checkbox         
3 - 310
15 - 29.5
60@190A
230/460
3
50/60
Trans Synergic 4000-C
Inverter
External
19.69 - 866.14
  checkbox checkbox checkbox checkbox       checkbox checkbox         
3 - 400
14.2 - 34
60@365A
230/460
3
50/60
Trans Synergic 5000- C
Inverter
External
19.69 - 866.14
  checkbox checkbox checkbox checkbox       checkbox checkbox         
3 - 500
14.2 - 39
60@450A
230/460
3
50/60
Trans Pulse Synergic 2700
Inverter
Built-in
19.69 - 866.14
  checkbox checkbox checkbox checkbox checkbox     checkbox checkbox         
3 - 270
14.2 - 27.5
60@210A
230/460
3
50/60
Trans Pulse Synergic 3200
Inverter
External
19.69 - 866.14
  checkbox checkbox checkbox checkbox checkbox     checkbox checkbox         
3 - 320
14.2 - 30
60@320A
230/460
3
50/60
Trans Pulse Synergic 4000
Inverter
External
19.69 - 866.14
  checkbox checkbox checkbox checkbox checkbox     checkbox checkbox         
3 - 400
14.2 - 34
60@365A
230/460
3
50/60
Trans Pulse Synergic 5000
Inverter
External
19.69 - 866.14
  checkbox checkbox checkbox checkbox checkbox     checkbox checkbox         
3 - 500
14.2 - 39
60@450A
230/460
3
50/60
Trans Pulse Synergic 2700 CMT
Inverter
Built-in
19.69 - 866.14
  checkbox checkbox checkbox checkbox checkbox     checkbox checkbox      checkbox  
3 - 270
14.2 - 27.5
60@210A
230/460
3
50/60

 HOBART WELDING PRODUCTS Troy, OH

Handler® 125 EZ
Rectifier
Built-in
50 - 500
        checkbox                   
125
29
20@90A, 19V
115
1
60
Handler® 140
Rectifier
Built-in
40 - 700
    checkbox   checkbox                   
25 - 140
28
20@90A, 19V
115
1
60
Handler® 187
Rectifier
Built-in
40 - 700
    checkbox   checkbox                   
25 - 185
31
30@130A, 21.5V
230
1
60
IronMan™ 210
Rectifier
Built-in
90 - 750
checkbox   checkbox   checkbox                   
30 - 210
33
40@150A, 23V
200/230
1
60
IronMan™ 250
Rectifier
Built-in
90 - 750
checkbox   checkbox   checkbox                   
30 - 250
35
60@200A, 24V
200/230
1
60
Handler® 210
Inverter
Built-in, opt. w/DP-3035 spool gun
60 - 770
    checkbox   checkbox                   
25 - 210
34
30@150A, 23V
230
1
60

 LIBURDI DIMETRICS CORP. Davidson, NC

Orbimig 450
Inverter
Orbital pipe weld head
Up to 1,000
    checkbox checkbox checkbox                   
450
20@450A
100
200/380/415/460/575
3
50/60

 LINCOLN ELECTRIC CO., THE Cleveland, OH

Power Mig 140C
Rectifier
Built-in
50 - 500
    checkbox   checkbox                   
30 - 140
19.5
20@90A, 19.5V
120
1
60
Power Mig 180C
Rectifier
Built-in
50 - 500
    checkbox   checkbox                   
30 - 180
20
30@130A, 20V
208/230
1
60
Power MIG 215
Rectifier
Built-in
50-700
checkbox   checkbox checkbox                     
30-250
40
30@215A, 22V
208/230
1
50/60
Power MIG 255C
Rectifier
Built-in
50 - 700
checkbox   checkbox   checkbox                   
30 - 300
40
40@250A, 26V
208/230/460/575
1
60
Power MIG 350 MP
Chopper
Built-in
50 - 700
checkbox checkbox checkbox checkbox checkbox checkbox   checkbox          checkbox  
5 - 350
76
60@300A, 32V
208/230/460/575
1
50/60
Invertec STT II
Inverter
External
      checkbox                    checkbox  
225
29
60
208/230/ 460
3
60
Invertec V350-PRO
Inverter
External
    checkbox checkbox checkbox checkbox checkbox   checkbox      checkbox     checkbox
350
34
60
200-230/ 380-575
1/3
50/60
Power Wave 355M
Inverter
External
    checkbox checkbox checkbox checkbox checkbox   checkbox            checkbox
350
34
60
200/208/230/ 380/400/415/ 460/575
1/3
50/60
Power Wave 455M / STT
Inverter
External
    checkbox checkbox checkbox checkbox checkbox   checkbox          checkbox checkbox
450
38
100
230/460/575
3
50/60
DC-400/600/655
Rectifier
External
    checkbox checkbox checkbox checkbox            checkbox checkbox   checkbox
400/ 600/ 650
36/ 44/ 44
100
230/460
3
60

 MAGNATECH LIMITED PARTNERSHIP East Granby, CT

MPS 4000
Inverter
On head, Push-pull
20 - 866
  checkbox checkbox checkbox checkbox checkbox checkbox               
400
70
50
200/230/460
3
50/60

 MILLER ELECTRIC MFG. CO. Appleton, WI

Millermatic 212
Tapped Transformer
Built-in
35 - 700
checkbox   checkbox checkbox                     
30 - 210
34.5
60@160A, 24.5V
200 (208)/ 230
1
60
Millermatic 350/350P
Inverter Solid State
All-in-One
50 - 700
checkbox   checkbox   checkbox checkbox                 
300
32
60
200/230/460
3
60
Invision 350 MPa
Inverter
External
50 - 780
    checkbox   checkbox checkbox          checkbox      
350
34
60
230 - 575
3
60
XMT 304 CC/CV
Inverter
External
    checkbox checkbox checkbox checkbox checkbox checkbox checkbox      checkbox     checkbox
5-400
10- 35
60@300A 60@225A
208/230/ 400/460/ 575
1/3
60
XMT 456 CC/CV
Inverter
External
    checkbox checkbox checkbox checkbox checkbox checkbox checkbox      checkbox     checkbox
5-600
10- 38
100@450A, 38V
230/ 460/575
3
60
XMT Series CC/CV
Inverter
External
    checkbox checkbox checkbox checkbox checkbox checkbox checkbox      checkbox     checkbox
5 - 600
10 - 38
60@350A, 60@300A, 100@450
208/230/400/460/ 575
1/3
60
Deltaweld 452
Solid-state
External
      checkbox checkbox              checkbox checkbox    
0-575
10- 38
100@450A, 38V
200-208/ 230/460, 230/ 460/575
3
60
Deltaweld 302
Solid-state
External
      checkbox checkbox                     
0-375
10- 32
100@300A, 32V
200-208/ 230/460, 230/ 460/575
3
60
Dimension 452
Solid-state
External
    checkbox checkbox checkbox checkbox            checkbox      
20-565
10- 38
100@450A, 38V
200 (208)/ 230/460 460/575
3
60
CP302
Mechanical Voltage Control
External
      checkbox checkbox                     
50-375
14- 44
100@300A, 32V
200/ 230/460
3
60

 PANASONIC FACTORY SOLUTIONS CO. Buffalo Grove, IL

GBII-350
Inverter
External
50 - 750
checkbox   checkbox   checkbox                   
35 - 350
36
60@350A
460
3
60
HMIII-350
Inverter
External
50 - 750
checkbox   checkbox   checkbox checkbox                 
35 - 350
36
60@350A
230/460
3
60
HMII-500
Inverter
External
50 - 750
checkbox   checkbox   checkbox checkbox                 
40 - 500
45
100@500A
460
3
60
Gunslinger 261
SCR
Internal
50 - 700
checkbox checkbox checkbox checkbox checkbox                   
40-260
38
40@260A
208/230/ 460/575
1
60
KF-350
SCR
External
50 - 750
checkbox   checkbox   checkbox                   
60 - 350
36
60@350A
230/460/575
3
60
KF-500
SCR
External
50 - 750
checkbox   checkbox   checkbox         &