Manual Powder Spray System Buyers' Guide©
System
Model
Number
Style
Spray Gun
Controller
Powder Feed
Output
Voltage
Range
(kilo-
volts)
Output
Current
Range
(micro-
amps)
Powder
Flow
Recipe
Fault
Display
Powder
Flow
Adjustment
ADVANCED POWDER COATINGS INC.
Denver, PA
MA2000
28
0 - 80
30 - 90
Corda 95
26
0 - 100
20 - 100
TS1
28
EXEL NORTH AMERICA INC.
West Chicago, IL
E-Series 400-D
18
0 - 85
0 - 100
E-Series 400-H
18
0 - 85
0 - 100
E-Series Lab Unit
18
0 - 85
0 - 100
ITW GEMA
Indianapolis, IN
Optiflex Box Unit
19
0 - 100
0 - 100
Optiflex Stirrer Unit
19
0 - 100
0 - 100
OptiFlex Fluidizer Unit
19
0 - 100
0 - 100
OptiFlex Cup Unit
30
0 - 100
0 - 100
OptiFlex Lab Unit
19
0 - 100
0 - 100
OptiFlex Wall Unit
19
0 - 100
0 - 100
JB FINISHING INC.
Bolton, ON
Canada
STAJET 406SAMES
630 kg
85
80
PARKER IONICS POWDER COATING SYSTEMS
Westland, MI
Parker I Ionics GX7000 Series
18.7
0 - 100
0 - 50
POWDER-X COATING SYSTEMS
Huntsville, AL
Eurotec 400-D
17
10 - 85
0 - 100
Eurotec 400-H
17
10 - 85
0 - 100
WAGNER SYSTEMS INC.
Elgin, IL
Bravo Airfluid-C Set
17.5
15 - 100
20 - 160
Bravo Airfluid-T Set
20.8
0 - 8
Bravo 50 L-C Set
17.5
15 - 100
20 - 160
Bravo 50 L-T Set
20.8
0 - 8
EPG-2008 Airfluid-C Set
17.5
40 - 160
EPG-2008 Airfluid-T Set
20.8
0 - 4
EPG-2008 50 L-C Set
17.5
20 - 100
40 - 160
EPG-2008 50 L-T Set
20.8
0 - 4
EPG-2008 CG Set
31.3
20 - 100
40 - 160
Contact us at: FMA Communications, Inc.
833 Featherstone Rd.
Rockford, IL 61107
815-399-8700
E-mail:
info@thefabricator.com
© 2008 FMA Communications, Inc. All rights reserved.
Privacy Policy
Legal Stuff
Site Map