Sheet titanium offers high corrosion resistance, weldability
August 07, 2007
Harvey Titanium Ltd., a division of Rolled Alloys, now offers CP-1 grade 4 and CP-3 grade 2 sheet titanium. Designed to offer high corrosion resistance and weldability, the titanium grades are available in thicknesses from 0.016 in. to 0.063 in.
Applications include CPI equipment, airframe components, cryogenic vessels, and condenser tubing.