In-die welding system welds nuts, screws at up to 60 SPM

September 12, 2006

In-die welding system welds nuts, screws at up to 60 SPM

OCON Automated Systems' in-die welding system is suitable for the integrated welding of nuts and screws while stamping with progressive, transfer, and tandem dies.

The system welds nuts and screws at up to 60 SPM and can utilize a user's specified elements to perform the task.