Extrusions can be tricky to bend and handle. Paying close attention to bender selection, die design, programming, and material handling can help to ensure efficient and productive bending.

Extrusions are everywhere—in conveyor systems, scaffolding, playground equipment, swimming pools, and furniture. They also are key components in architectural windows and automotive window trim. We are surrounded by bent extrusions and their close cousins, bent rolled formed sections.

Managing the flow of an extrusion within the bend zone is at the heart of making a good bend. Die clearance, die material, die hardness, and die surface finish can all align to produce quality bends.

The bend radius and the compressive forces within the workpiece are inversely proportional. In other words, as the bend radius decreases, the compressive force increases. This influences bender choice. Large-radius bends generally are well-suited to either a roll bender or a stretch bender. Tight-radius bends often require a rotary draw bender.

The compressive forces also influence die design. As the compressive forces increase, the tooling requirements become more critical because the forces tend to cause thin cross sections to buckle. The tooling's design often is the most critical factor.

Common Die Designs

Consider a simple L channel with a leg-out bend (see Figure 1).

As the L channel is drawn around the bend die, the outer section of the leg is in tension.

Now take the same cross section and turn the leg in (see Figure 2).

In this case, the inner fibers of the leg are in compression and have a tendency to buckle as the bend radius becomes smaller.

Too much clearance in the gap (G) can lead to buckling. Too little clearance prevents the extrusion from flowing freely in the die as it rotates through the bend. As the material thickness (T) decreases, the tolerance of the gap becomes more critical.

Even with the right gap, the surface finish of the die can start to break down, resulting in galling. As the abrasiveness of the workpiece increases, the likelihood of breakdown and galling also increases.

Now consider adding another leg. This is a U channel (see Figure 3).

Bending the U channel with legs in highlights the importance of material growth during bending. As the material rotates about the bend die, the height (H) of the extrusion grows noticeably.

Some extrusions need more than one bend radius in a single part. This requires several bender setups or a bender that supports more than one bend radius. Some CNC benders are equipped for these sorts of bends — they have right-hand and left-hand bending capability and use a dual-radius split die actuator.

Material Handling

In some cases—especially long, thin sections with several bends—the material's stiffness isn't sufficient to support the weight of the bent material after it exits the bender. The material acts like a wet noodle and requires continuous support. Support systems vary from very simple, a table, to complex, such as a microprocessor-controlled material handling system integrated with the bender's controller (see Figure 4).

Programming Bends

Programming a simple one- or two-bend part doesn't take long. However, programming a complex part with several bends can take quite a bit of time. Some modern software tools can simplify the programming.

For example, back-to-back bends usually require a 180-degree plane rotation between the bends. Many extrusions are flimsy, making this an awkward and occasionally difficult task. A right-hand/left-hand bender can bend in both directions, which makes bending easier. However, the programming isn't any easier.

A bender that can read the extrusion's profile directly from a CAD program nearly eliminates programming time. Importing a STEP file derived from a solid model can program the bender in less than a second. After importing the length, rotation, and angle (LRA) data and centerline radius information, the software identifies the CLR of a specific bend, sets up the tooling, determines bend direction, and queries its database of similar materials to try to predict the springback percentage.

The operator then selects a standard tool package from a software library.

A tool package might include the pressure die length, clamp die length, bend die information, material handling setup information, and various pressure settings.

Disadvantages

The initial cost to bring online the software tools for programming can be a limiting factor for some shops. Also, investing in a machine that doesn't have a dual stack feature can increase the time it takes to see a return on an investment.


George Winton
founder and president,
Winton Machine Co.

George Winton is the founder and president of Winton Machine Co., 3644 Burnette Road, Suwanee, GA 30024, 888-321-1499, www.wintonmachine.com.





How Do you Rate This Article?            
Poor 5  Great

Comments:

Email address (optional):

Want more information?

Learn more about this company:

Tube and pipe fabrication technical articles


 
  • Sponsors
  • Magnatech Limited Partnership
  • Scotchman Industries Inc.
  • AltaMAR
  • BLM -- tube and pipe fabrication
Fabricators and Manufacturers Association, International Tube and Pipe Association, International