Exclusive to thefabricator.com

Tube mill cutoff die setup for square and rectangular profiles

By John J. Pavelec, Contributing Writer
September 13, 2005

When properly selected and utilized, single-cut die sets can produce top-quality cut ends on square and rectangular tubing. This article discusses the criteria for selecting and using the die sets to achieve the best results.

Modern high-speed tube mills produce square and rectangular tubing very efficiently. They typically reshape square and rectangular tube from a welded round in the sizing section of the mill (Figure 1).

Figure 1
Tube Mill Cutoff - Left to Right - Single Cut
Figure 2
Single-Cut Master Die Set

The vertical and horizontal orientation of the final shape is located on the centerline of the equivalent welded round tube. The weld can be positioned in the corner or anywhere along the flat of the shape.

Squares

Heavy-duty single-cut master die sets are the best choice for cutting square tubing.

Orienting the master die set so that the shear blade path is through the diagonal corners of the square tubing as shown in Figure 2 is preferable. This orientation produces very little end-cut distortion.

The shear blade and die jaw layout should be arranged as shown in Figure 3. The shear blade tip should enter the top corner of the tube at the center of its radius. A 120-degree included angle blade tip provides the best shear angle and results in very little end-cut distortion.

Figure 3
Single-Cut Blade and Jaw Arrangement
Figure 4
Blade Lubrication
Figure 5
Corner Match

Blade-to-die-jaw clearances are the same as with rounds. Start with 10 percent of the tube wall thickness for mild steel tube.

Proper blade lubrication (Figure 4) is critical to reliable, top-quality performance. High-quality cutting lubricant should be applied to the working surfaces of the shear blade before each cut.

The tube's corner radii will vary with changes in the material thickness and welded tube size before reshaping in the tube mill sizing section. For a clean cut with minimum distortion and burr, the corner radii in the supporting die jaws should match the tube corner radii (Figure 5). This requires separate die jaw sets to match each tube corner radii change.

Expect a dimensionally correct, clean-cut tube when the die jaws conform properly to the shape (Figure 6).

Figure 6
Square End Cut
Figure 7
Large Corners
Figure 8
Corner Burr

Excessive burrs will develop in the side and bottom corners if the tube radii are larger than the supporting die jaw radii (Figures 7 and 8).

Rectangles

Heavy-duty single-cut master die sets are the best choice for rectangular tubing (Figure 9).

Like square tubing, a rectangular tube typically is reshaped in the sizing section of the tube mill around the centerline of the equivalent welded round. The rectangle orientation varies with the required position of the weld seam. In any case, the rectangle should be oriented with corners at or near the vertical plane.

Figure 9
Single-Cut Master Die Set
for Rectangular Tubing
Figure 10
Rectangle Layout
Figure 11
Rectangle End Cut

The shear blade tip can be offset, if necessary, to line up with the center of the rectangle's top corner. The blade tip's included angle varies with the tube's orientation. A sharp radius tip instead of a sharp pointed tip suits a wide range of corner radii with excellent results. The layout shown in Figure 10 produces a clean cut with little distortion (Figure 11).

Simple, inexpensive, heavy-duty single-cut die sets can produce top-quality cut ends on square and rectangular tubing. The die jaws selected for each shape must conform to the shape in all respects, especially the corner radii, for best results. Well-lubricated shear blades with tip configurations that ensure proper shear angles and tip alignment can provide tens of thousands of cuts between regrinds.

 

John J. Pavelec is vice president of BetaRam Inc.,
P.O. Box 334, Troy, MI 48099, 248-853-0446,
brsales@betaram.com,www.betaram.com
.

 

 


TAGS: betaram, corner radii, john pavelec, pipe, pipe production, rectangular tube, shear blades, square tube, tube, tube cutoff die sets, tube cutting, tube production




How Do you Rate This Article?            
Poor 5  Great

Comments:

Email address (optional):

Want more information?

Learn more about this company:

Related Links:

  • Fraunhofer ILT believes a fabricating operation can reduce its operating costs by a factor of two or more when applying this dual-use technology.
  • Taking into account the combi-head's technical features and capabilities, Fraunhofer ILT believes a fabricating operation can reduce its operating costs by a factor of two or more when applying this dual-use technology.

Tube and pipe production technical articles


 