The Scotch-Brite™ radial bristle disks and brushes from 3M are designed for industrial applications, such as cleaning metal before welding, removing discoloration and sealant, and deburring, without damaging the underlying surface. The plastic rotary tools are embedded with the company's Cubitron™ abrasive grain.
The flexible, lightweight tools are available in three sizes: 4.5-in. discs and 6-in. and 8-in. brushes. They contain no wire filaments and are solvent-free.