AK Steel announces February surcharges

AK Steel has advised its flat-rolled carbon steel customers that a $196 per ton surcharge will be added to invoices for products shipped February 2005, a decrease of $9 from January's surcharge of $205 per ton. The company also advised its electrical steel customers that a $410 per ton surcharge will be added to invoices for electrical steel products shipped in February, an increase of $10 from the January surcharge of $400 per ton for those products. February surcharges for all stainless steel products the company produces can be found on its Web site.