Arco Industries LLC copper-nickel alloy electrode 813 exhibits high corrosion resistance, especially against salt water, the company says.
The ERCuNi electrode primarily is used for welding 70/30, 80/20, and 90/10 copper-nickel alloy and is designed for joining nickel-copper alloys and Nickel 200 to copper-nickel alloys.