May 9, 2006
The 50-ton, five-station Geka Bendicrop ironworker from Comeq Inc. features a full structural die block and quick-change tooling. It has a built-in bending station.
Bending length is 4 in. with a maximum capacity of 3/8 in. thick; plate shear capacity is 14 by in.; angle shear capacity is 3 by 3 by 5/16 in.; round bar capacity is 1 3/8 in.; square bar capacity is 1 3/16 in.; and notcher capacity is in.