ESAB Welding & Cutting Products has introduced the Atom Arc 7018 Acclaim stick electrode. According to the manufacturer, the electrode has the same drive and dig as its original Atom Arc stick electrode, with improved weld puddle control for simplified out-of-position welding.

The electrode provides a deep, penetrating arc and a wide operating range. It meets E7018H4R classification.