August 9, 2012

Goff's Enterprises has added weld blankets to its product line. The lightweight, flexible weld blankets are designed to be draped over materials, equipment, vehicles, and vehicle interiors to provide protection from welding and grinding sparks, molten and hot metal debris, and torch cutting spatter.
Able to withstand heat up to 1,800 degrees F, the weld blankets are constructed with a tear-resistant, soft carbon fiber material. They are stock sized at 80 by 72 in. and packaged in a reusable container.