Hypertherm will unveil new edge profiling technology at FABTECH designed to help fabricators and CNC table manufacturers achieve accurate bevel cuts. The technology includes factory-tested mild steel cut charts for the manufacturer's HyPerformance HPRXD plasma systems. These cut charts contain parameters that help reduce the amount of time and effort required to produce bevels using plasma.
The company plans to embed the cut charts in its CNC/CAM software and make it available to its partners for inclusion with their proprietary CNC/CAM programs.