February 22, 2011

Jet Edge’s High Flow Abrasivejet delivers up to 3.5 lbs./min. of abrasive and up to 8.6 GPM of ultrahigh-pressure water for abrasive waterjet cutting applications.
The cutting head is suitable for making separation cuts in steel plates or pipes. It can operate at up to 55,000 PSI and is suited for use with lower-pressure, high-flow waterjet pumps. It can be used with any manufacturer's waterjet system.