La-Co Industries has developed the MarkalĀ® Pro-Line WP industrial-grade liquid paint marker. Engineered with a permanent, fast-drying, low-VOC formula, the marker resists spreading when in contact with water or water-based liquids.

Low in halogenated compounds and sulfur, the marker uses a low-corrosive formula that is safe for use on stainless steel and other superalloys. It marks on iron, carbon steel, aluminum, powder coating, PVC plastics, coding alloys, nonferrous metals, textile, and rubber.