Osborn offers the Welders Choice™ line of finishing products designed for professional welding applications.
The stringer bead brushes, including the refined TY™ encapsulated stringer bead brushes, clean J-weld joints. Improved elastomers in the narrow-face, aggressive knots make the brushes suitable for cleaning stringer bead welds.
The scratch brushes are made with kiln-dried hardwood for tuft retention, even in severe applications. The wire fill provides superior cutting ability and fatigue resistance, according to the manufacturer.
The cup brushes, including the TY encapsulated cup brushes, mount on portable and electric tools and finishing machines and are suitable for surface prep and burr removal, as well as other surface work.