A line of abrasive grinding wheels for removing heavy welds from stainless, mild, and carbon steel with minimal vibration is available from Rex-Cut Products Inc.
Rex-Cut® Sigma-Green grinding wheels feature a blend of zirconia and ceramic abrasives with a proprietary elastomer bond that promotes low vibration and smooth operation for applications requiring heavy stock removal.
Offered in 36-, 46-, and 60-grit styles, the wheels are available in 4- , 4-1/2- , 5- , and 7-in. sizes, with or without hubs, for right-angle grinders. A 5/8-11 throw-away adapter that screws onto a standard 5/8-in. arbor is optional.