Rex-Cut Products' Rex-Cut® Grind and Blend Kit removes heavy welds on stainless steel and aluminum.
The kit includes a Sigma Green wheel featuring a zirconia-ceramic grain and proprietary bonding for grinding out cracks and removing welds. The cotton fiber Type 27 blending and finishing wheel leaves a 32 RMS or better finish on stainless steel. Two 4 -in.-dia. wheels are included with or without hubs.