Warm forming magnesium, aluminum tubes

October 3, 2006 | By Yingyot Aue-u-lan, Jon Ander Esnaloa, David Guza, Taylan Altan, Ph.D.

Research shows that in forming lightweight materials such as aluminum and magnesium alloys, the formability increases as the temperature increases, especially in the range from 200 degrees C to 300 degrees C (392 degrees F to 572 degrees F).1-5 The Center for Precision Forming (CPF, formerly...