Bending tube or pipe successfully is a matter of managing a handful of processes and variables and controlling the flow of the metal. The same principles apply to bending profiles, or rolled steel sections (RSS). However, because profiles aren't closed, they are more prone to distortion than tube or pipe. A close look at an RSS bending job provides a step-by-step approach for tackling this sort of project.