Laser cutting

Air cutting revisited

March 13, 2007

By: ,

Fabricators are increasingly using compressed air in laser cutting, instead of relying on laser assist gases such as oxygen and nitrogen. Recent findings reveal that shop air can be used on more material types and thicknesses, including parts on which the edge quality is visible.

Continue Reading

A breath of fresh air

August 8, 2006

By: ,

Two standard laser assist gases are oxygen and nitrogen. However, a third gas — shop air — has become a viable alternative.