Testing and Measuring | Articles | The FABRICATOR

Inspecting and verifying fillet weld size

May 19, 2009 | By Joe Pavilanis

Woolf Aircraft Products Inc. developed an inspection tool that can beused to measure a leg length, as well as the actual throat of a weld.Using these two known measurements, quality assurance personnelthen can determine the actual size and the convexity and concavity ofa specific fillet weld.

Continue Reading