High School Career Center in Texas

Marty Rice

Contributing Writer
High School Career Center in Texas



Marty Rice is a welding instructor at a high school career center in Texas. He is an honorary member of the Ironworkers Local 263.

 

Questions for the author can be e-mailed to vickib@thefabricator.com

Arc Welding | Articles

Lessons learned in a welding career

May 13, 2015 | By Marty Rice

The importance of saving money and of being safe on the job are among the lessons welding instructor Marty Rice learned throughout his welding career. Among those who taught him these lessons was Charlie.

Continue Reading

Arc Welding | Articles

Friendship and loss on the job

December 3, 2014 | By Marty Rice

A young ironworker learns the value of job friendships, how to make work fun, and how devastating an on-the-job accident can be.

Continue Reading

Arc Welding | Articles

Arc Welding 101: Wire-feed welding, stick welding with the same machine

November 17, 2014 | By Marty Rice

Q: I would like to know if a wire-feed welding machine can double as a modest-amperage DC shielded metal arc welding (SMAW) machine if I attach an electrode holder to the output. I have been told that aluminum welding works well and is convenient using SMAW and DC. I have the aluminum roller kit...

Continue Reading

Arc Welding | Articles

Arc Welding 101: Advice for MIG welding a motorcycle frame

November 14, 2014 | By Marty Rice

Q: I just ran across the article you wrote about gas metal arc welding (GMAW) machines in the July/August 2004 issue of Practical Welding Today. Your article was very informative. I will be purchasing a welding machine soon and would like to know if a GMAW machine can handle a motorcycle frame. Any...

Continue Reading

Arc Welding | Articles

Arc Welding 101: Electrodes and machine settings

November 13, 2014 | By Marty Rice

Q: I know how to arc weld. I took arc welding classes in high school and was certified in the state of California. Unfortunately, they never taught me about the settings and what electrodes were best for what jobs. For example, I’m rebuilding a motorcycle and I want to straighten a minor bend...

Continue Reading

Arc Welding | Articles

Arc Welding 101: Blowing out metal when welding car panels

November 12, 2014 | By Marty Rice

Q: I only have a 110-V arc welding machine, and I want to weld car panels, but I keep blowing out the metal. What can I do to stop this? Can I use aluminum rods? Dan F. A: You can use aluminum rods on aluminum only, and they typically are used only for really thick pieces, about 0.25 inch and...

Continue Reading

Arc Welding | Articles

Arc Welding 101: Advice for a first-time welder

November 11, 2014 | By Marty Rice

Q: I’m thinking about learning how to weld. I want a gas metal arc welding (GMAW) machine so I can box my 1955 GMC truck frame and install an independent front suspension. Where should I start? William S. A: Books, the Internet, videos, cable TV shows, and classes offer more information about...

Continue Reading

Arc Welding | Articles

Arc Welding 101: Don't spare the rod—Electrode storage myths

November 10, 2014 | By Marty Rice

Welders often ask me, “Can I dry welding rods in my oven if they have gotten wet?” and “Can I put 7018 welding rods in my freezer for a certain amount of time if they are old?” The 7018 electrode is a low-hydrogen rod, which means it doesn’t tolerate moisture in its flux. If you’ve...

Continue Reading

Arc Welding | Articles

Arc Welding 101: Hot rods and MIG

November 7, 2014 | By Marty Rice

Q: Can gas metal arc welding (GMAW) be used on motorcycles and hot rods? A: Yes, but it takes a lot more than just running a good bead. The popularity of cable TV fabrication shows with the likes of Jesse James, the Teutuls, and Boyd Coddington has generated a lot of questions about GMAW....

Continue Reading

Arc Welding | Articles

Arc Welding 101: Thoriated tungsten and its alternatives

November 6, 2014 | By Marty Rice

Q: In "TIG welding--An overview," you said you used 2 percent thoriated tungsten until you heard about the health risks. What are other options? Does cost vary significantly (not that cost should matter when it comes to health or safety)? My fabrication shop runs 14 gas tungsten arc welding (GTAW)...

Continue Reading

Arc Welding | Articles

Arc Welding 101: Uphill MIG

November 5, 2014 | By Marty Rice

Q: What patterns is used in uphill gas metal arc welding (GMAW), and what amperage should I use on 0.25-in. plate using 75 percent argon/25 percent carbon dioxide shielding gas? Where I work—I build farm equipment—there’s no need for uphill welding, so I like to practice at lunch. August F....

Continue Reading

Arc Welding | Articles

Arc Welding 101: How to motivate a welder

November 4, 2014 | By Marty Rice

Many people have asked me how to motivate welders in the shop. The following are some ideas. Money. If a shop doesn’t pay well, it won’t attract good welders. Health benefits and a 401(K) plan show that a company cares about its employees. Safety. Shops must be safe to work in; every worker,...

Continue Reading

Arc Welding | Articles

Arc Welding 101: Best practices for aluminized steel

November 3, 2014 | By Marty Rice

Q: Which process, filler rod, and shielding gas work best for welding aluminized steel? A: Aluminized steel resists fire, heat, corrosion, and oxidation. It’s used in many applications, such as weather shielding and exhaust systems. Steel is hot-dipped in an aluminum solution, which provides...

Continue Reading

Arc Welding | Articles

Arc Welding 101: Preparing for an overhead certification test

October 31, 2014 | By Marty Rice

Q: A carpenter friend of mine has taken some night-school welding courses and needs help getting certified in overhead welding. He uses steel beams to support the homes he builds and would like to weld them himself. How should he prepare for and take an overhead welding certification test?...

Continue Reading

Arc Welding | Articles

You’re fired!

April 8, 2014 | By Marty Rice

You may have the skills, but if you can’t follow rules and don’t have a good work ethic, your skills won’t get you very far. Marty Rice shares personal stories of workers who have learned this lesson the hard way.

Continue Reading