Tony has a background as a certified welding inspector, welding engineer-quality manager, and NDT manager. He also serves as chairman of The Aluminum Association Technical Advisory Panel for Welding and Joining, vice chairman of the AWS D1G Subcommittee 7 on Welded Aluminum Structures, and a member of Practical Welding Today's Editorial Review Committee.
alloy welding aluminum

Welding aluminum

June 30, 2009

By:

The first step in learning about welding aluminum is learning about the various alloys themselves (cast and wrought)—the digits used in the aluminum designation system, the properties of the various alloys, and the considerations in matching a filler metal to a base material.

Continue Reading

alloy content crack sensitivity

Finding an ally alloy

May 15, 2009

By:

Choosing the best filler metal for aluminum welding involves takinginto account the operating conditions of the finished weldedcomponent as well as six important variables that can affect theoperating condition.

Continue Reading

Arc welding image

Quality inspections

July 10, 2007

By:

To ensure quality welds, it is important to have a quality weld inspection program in place. In order to do so, a company must understand how to evaluate weld characteristics, determine weld quality, and have a welding inspector capable of performing a number of different testing methods.

Continue Reading

Understanding weld discontinuities

June 12, 2003

By:

A welder's primary concern in any kind of work is ensuring his weld is sound. For this reason, it's important for an inspector examining the weld to be able to spot a variety of weld discontinuities, including:Porosity.Incomplete fusion.Incomplete joint penetration.Unacceptable weld...

Continue Reading

Establishing quality systems for welding

May 16, 2002

By:

Welding codes and standards exist for a reason. They provide a framework for welders and shop managers to keep quality a top priority in their work.

Continue Reading

Inspection Connection: Radiographic and ultrasonic weld inspection

February 14, 2002

By:

This article outlines the differences in radiographic and ultrasonic weld inspection, the two most common methods if nondestructive testing. It gives an overview of both methods, including how they are used.

Continue Reading

What welding inspectors should know about welding codes and standards

January 24, 2002

By:

Many aspects of welded component design and fabrication are governed by documents known as codes and standards.

Continue Reading

Radiographic and ultrasonic weld inspection

December 13, 2001

By:

This article outlines the differences in radiographic and ultrasonic weld inspection, the two most common methods if nondestructive testing. It gives an overview of both methods, including how they are used.