Advanced materials require advanced knowledge

November 8, 2005 | By Jerry E. Gould, Warren Peterson

Given the range of advanced high-strength steels to be introduced into automotive bodies over the next decade, automakers must recognize the implication of non-traditional resistance spot weld failure modes.