Characteristics |
Chemistry % |
Application Method |
Type or Operation |
Cleaning
Method |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
 |
CHEMTOOL INC.
Crystal Lake, IL
United States
|
| ReNu 900 |
 |
 |
70 |
0 |
30 |
0 |
|
 |
 |
 |
|
 |
 |
 |
|
 |
|
 |
|
|
 |
|
| ReNu 920 |
 |
 |
90 |
0 |
10 |
0 |
|
 |
 |
 |
|
 |
 |
 |
|
|
|
 |
|
 |
 |
 |
| ReNu 9500 |
 |
 |
95 |
0 |
5 |
0 |
|
 |
 |
 |
|
 |
 |
 |
|
 |
|
|
|
|
 |
 |
| ReNu 9800 |
 |
 |
80 |
0 |
20 |
0 |
|
|
 |
 |
|
|
|
 |
|
 |
|
|
 |
 |
 |
 |
| ReNu FGEP |
 |
 |
90 |
0 |
10 |
0 |
|
|
|
 |
|
 |
|
|
|
 |
|
|
|
 |
 |
 |
| CT 492 |
 |
 |
100 |
0 |
0 |
0 |
 |
 |
 |
 |
|
 |
 |
 |
|
|
|
 |
|
|
 |
 |
| Novus AW Hydraulic |
 |
 |
92 |
0 |
8 |
0 |
|
|
|
 |
|
|
|
|
 |
|
|
|
|
|
|
 |
| Novus FR Hydraulic |
 |
 |
95 |
0 |
5 |
0 |
|
|
|
 |
|
|
|
|
 |
|
|
|
|
|
|
 |
| Novus FG Hydraulic |
 |
 |
90 |
0 |
10 |
0 |
|
|
|
 |
|
|
|
|
 |
|
|
|
|
|
|
 |
| Novus THF Tractor Hyd |
 |
 |
65 |
0 |
35 |
0 |
|
|
|
 |
|
|
|
|
 |
|
|
|
|
|
|
 |
| Novus FG Gear |
 |
 |
90 |
0 |
10 |
0 |
|
|
|
 |
|
|
|
|
|
|
 |
|
|
|
|
 |
| ReNu Earthsolv |
 |
 |
100 |
0 |
0 |
0 |
|
 |
 |
 |
|
 |
 |
 |
|
|
|
 |
|
|
 |
 |
| ReNu SoyPlus |
 |
 |
85 |
0 |
15 |
0 |
|
 |
 |
 |
|
 |
 |
 |
|
|
|
 |
|
|
 |
 |
| Elimicote Clear Choice |
 |
 |
85 |
0 |
15 |
0 |
|
 |
 |
 |
|
 |
 |
 |
|
|
|
 |
|
|
 |
 |
CIMCOOL FLUID TECHNOLOGY
Cincinnati, OH
United States
|
| CIMFREE VG-990M |
|
 |
|
0 |
0 |
0 |
|
|
 |
|
|
|
|
|
|
|
|
 |
|
|
 |
|
| CIMFREE VG901ZH |
|
 |
|
0 |
0 |
0 |
|
|
 |
|
|
|
|
|
|
|
|
 |
|
|
 |
|
| CIMFREE VG-S175 |
|
 |
|
0 |
0 |
0 |
|
|
 |
|
|
|
|
|
|
|
|
 |
|
|
 |
|
| CIMFREE VG-S110P |
|
 |
|
1 |
1 |
0 |
 |
|
 |
|
|
|
|
|
|
|
|
 |
|
|
 |
|
| CIMFREE VG-MF5350 |
|
 |
|
0 |
0 |
0 |
|
|
 |
 |
|
|
 |
|
|
 |
|
|
|
|
 |
|
| CIMFREE VG-703ES |
|
 |
|
0 |
0 |
0 |
 |
|
|
|
|
|
|
|
|
|
|
 |
|
|
 |
|
| CIMFREE VG-3900H |
|
 |
|
0 |
0 |
0 |
|
|
 |
|
|
|
|
|
|
|
|
 |
|
|
 |
|
| CIMFREE VG-920M |
|
 |
|
0 |
0 |
0 |
|
|
 |
|
|
|
|
|
|
|
|
 |
|
|
 |
|
ENVIRONMENTAL LUBRICANTS MANUFACTURING INC.
Grundy Center, IA
|
| ELM EP Premium Lithium Complex Grease #2 |
 |
|
>50 |
|
<40 |
|
|
|
|
 |
|
|
|
 |
|
|
|
|
|
|
|
 |
| ELM EP Plus Lithium Grease #2 |
 |
|
>75 |
|
|
|
|
|
|
 |
|
|
|
 |
|
|
|
|
|
|
|
 |
| ELM Food Machinery Grease #2 |
 |
|
>95 |
|
|
|
|
|
|
 |
|
|
|
 |
|
|
|
|
|
|
|
|
| ELM Multipurpose Lubricant |
 |
|
>95 |
|
|
|
 |
 |
 |
 |
|
|
|
 |
|
 |
|
 |
 |
 |
|
|
| ELM Penetrating Fluid |
 |
|
>90 |
|
|
|
 |
 |
 |
 |
|
|
|
 |
|
|
|
|
|
|
|
|
| ELM Food-grade Chain and Cable Lubricant |
 |
|
>95 |
|
|
|
 |
 |
 |
 |
|
|
|
 |
|
|
|
|
|
|
|
|
| ELM Food-grade Hydraulic Oil ISO 32/46 |
|
|
>95 |
|
|
|
|
|
|
 |
|
|
|
 |
|
|
|
|
|
|
|
|
| ELM Industrial Hydraulic Oil (ISO 32/46/68) |
 |
|
80-98 |
|
|
|
|
|
|
 |
|
|
|
 |
|
|
|
|
|
|
|
|
| ELM Universal Tractor Hydraulic Oil |
 |
|
>70 |
|
|
|
|
|
|
 |
|
|
|
 |
|
|
|
|
|
|
|
|
| ELM Hydraulic Jack Oil |
 |
|
>70 |
|
|
|
|
|
|
 |
|
|
|
 |
|
|
|
|
|
|
|
|
| ELM Bar and Chain Oil |
 |
|
>90 |
|
|
|
|
|
|
 |
|
|
|
 |
|
|
|
|
|
|
|
|
| ELM Rust and Corrosion Inhibitor |
 |
|
>80 |
|
|
|
 |
 |
 |
 |
|
|
|
 |
|
|
|
|
|
|
|
|
| ELM Air Tool Oil |
 |
|
>75 |
|
|
|
|
 |
 |
 |
|
|
|
 |
|
|
|
|
|
|
|
|
| ELM Gear Oils |
 |
|
>75 |
|
|
|
|
|
|
 |
|
|
|
 |
|
|
 |
|
|
|
|
|
ETNA PRODUCTS INC.
Chagrin Falls, OH
United States
|
| MASTERDRAW® B1619 with EELT™ |
|
 |
15 |
1 |
|
|
|
|
 |
|
|
|
|
|
|
 |
|
|
|
|
 |
|
| MASTERDRAW® EBE 110 |
|
 |
98 |
0 |
0 |
|
 |
|
 |
|
|
|
|
|
|
 |
|
|
 |
|
 |
|
| MASTERDRAW® SYN G |
|
 |
75 |
0 |
0 |
|
 |
 |
 |
 |
|
|
 |
 |
|
 |
 |
|
|
|
 |
|
| MASTERDRAW® MQL 934 |
 |
|
100 |
0 |
0 |
|
 |
|
|
|
|
|
|
|
|
|
|
 |
|
|
|
|
| MASTERDRAW® MQL 995B |
|
|
80 |
0 |
0 |
|
 |
|
|
|
|
|
|
|
|
|
|
 |
|
|
|
|
| MASTERALL® SYN 12 |
|
 |
65 |
0 |
0 |
|
|
|
 |
|
|
|
|
|
|
|
|
 |
|
|
|
|
ETNA-BECHEM LUBRICANTS LTD.
Chagrin Falls, OH
United States
|
| Bechem Eco P-way Lube |
 |
|
|
0 |
0 |
|
|
|
|
|
|
|
|
|
|
|
|
 |
|
|
|
|
| Bechem Berugear UWS FG 34-00 |
 |
|
|
0 |
0 |
|
|
|
 |
|
|
|
|
|
|
|
 |
|
|
|
|
|
| Bechem Unopol S623U |
|
 |
|
0 |
0 |
|
|
|
 |
|
|
|
|
|
|
 |
|
|
|
|
|
|
| Bechem Hydrostar Series |
 |
|
|
0 |
0 |
|
|
|
 |
|
|
|
|
|
|
|
 |
|
|
|
|
|
FUCHS LUBRICANTS CO.
Harvey, IL
United States
Fuchs products are inherently biodegradable. Fuchs does not warrant that the products satisfy a specific standard of biodegradability, nor that the products are suitable for disposal as a raw effluent. As always, users of industrial lubricants should evaluate their waste streams independently and determine appropriate disposal according to applicable regulations.
|
| Eco Draw HVE-1 |
 |
 |
100 |
0 |
0 |
0 |
|
 |
 |
 |
|
|
 |
|
|
 |
|
|
|
|
 |
|
| Eco Draw HVRG-8 |
 |
 |
100 |
0 |
0 |
0 |
|
 |
 |
 |
|
|
 |
|
|
 |
|
|
|
|
 |
|
| Eco Draw HVRG-4WP |
 |
 |
100 |
0 |
0 |
0 |
|
 |
 |
 |
|
|
 |
|
|
 |
|
|
|
|
 |
|
| Eco Draw HSS 2900 |
 |
|
75 |
|
|
|
 |
 |
 |
 |
|
|
 |
|
|
 |
|
|
 |
 |
 |
|
INTERNATIONAL CHEMICAL CO.
Philadelphia, PA
United States
|
| IC 2502 |
 |
 |
85 |
0 |
15 |
0 |
|
 |
 |
 |
|
|
 |
|
|
 |
|
 |
|
|
 |
|
| IC 1599-P2 |
 |
 |
70 |
|
30 |
0 |
|
|
|
|
|
|
 |
|
|
|
|
|
 |
|
|
|
| IC 2801-DL |
|
 |
75 |
25 |
|
0 |
|
|
|
|
|
 |
|
|
|
 |
|
|
|
 |
|
|
IRMCO LEANGREEN METALFORMING
Evanston, IL
United States
Irmco products are readily biodegradable, an expectation based on available component data or QSAR model.
|
| 090-000 |
 |
 |
20 |
0 |
25 |
0 |
 |
 |
 |
 |
|
|
 |
 |
|
 |
|
 |
 |
|
 |
|
| 245-000 |
 |
 |
100 |
0 |
0 |
0 |
 |
 |
 |
 |
|
|
 |
 |
|
 |
|
 |
|
|
|
 |
| 980-000 |
 |
|
10 |
0 |
10 |
0 |
|
|
 |
 |
|
|
|
|
|
 |
|
 |
|
|
 |
|
JOHN NEALE LTD.
Halesowen,
United Kingdom
|
| Superdraw SE4000 |
 |
|
100 |
0 |
0 |
0 |
|
|
 |
 |
|
|
 |
|
|
 |
|
|
|
|
|
 |
| Envirocut ML40 |
 |
|
100 |
0 |
0 |
0 |
 |
 |
 |
|
|
|
|
|
|
 |
|
 |
 |
 |
|
 |
| Hydraulic SE46 |
 |
|
99 |
0 |
1 |
0 |
|
|
 |
|
|
|
|
|
|
|
|
|
|
|
|
 |
| Coating Lubricant CR-special |
 |
|
95 |
0 |
0 |
5 |
|
|
|
|
 |
|
|
|
|
 |
|
|
|
 |
|
 |
| Gear Oil SE220 |
 |
|
99 |
|
1 |
|
|
|
 |
|
|
|
|
|
|
|
 |
|
|
|
 |
 |
| Envirocut SE10 |
 |
 |
100 |
|
|
|
 |
 |
 |
 |
|
|
|
 |
|
 |
|
 |
 |
 |
 |
 |
LAMSON OIL CO.
Rockford, IL
United States
|
| MeterLube |
 |
|
100 |
|
|
|
 |
 |
|
 |
|
|
 |
 |
|
 |
|
 |
 |
 |
 |
 |
| LamSyn |
 |
|
75-100 |
|
0-25 |
|
 |
 |
|
 |
|
|
 |
|
|
 |
|
 |
|
 |
 |
|
| Eco Vanish Series |
 |
 |
100 |
|
|
|
 |
 |
|
 |
|
|
 |
|
|
 |
|
 |
|
 |
 |
|
METALLOID CORPORATION
Sturgis, MI
United States
|
| ADDVANCE 6110 |
 |
|
70 |
0 |
0 |
0 |
 |
 |
 |
 |
|
|
|
|
|
 |
|
|
|
|
 |
|
| ADDVANCE 6120 |
 |
|
60 |
0 |
0 |
0 |
 |
 |
 |
 |
|
|
 |
|
|
 |
|
|
|
 |
 |
|
| Microlubricant MQL-350 |
 |
 |
90 |
0 |
0 |
0 |
 |
 |
 |
 |
|
|
|
|
|
|
|
 |
|
 |
|
 |
| ADDVANCE 5140 |
 |
 |
100 |
0 |
0 |
0 |
 |
 |
 |
 |
|
|
 |
|
|
 |
|
 |
|
|
 |
|
| ADDVANCE 5270 |
 |
 |
100 |
0 |
0 |
0 |
 |
 |
 |
 |
|
|
 |
|
|
 |
|
 |
|
|
 |
|
| ADDVANCE 6040 |
 |
 |
100 |
0 |
0 |
0 |
 |
 |
 |
 |
|
|
 |
|
|
 |
|
 |
|
|
 |
|
| ADDVANCE 6090 |
 |
 |
100 |
0 |
0 |
0 |
 |
 |
 |
 |
|
|
 |
|
|
 |
|
 |
|
|
 |
|
| ADDVANCE 6110 HV |
 |
 |
100 |
0 |
0 |
0 |
 |
 |
 |
 |
|
|
 |
|
|
 |
|
 |
|
|
 |
|
| ADDVANCE 6120 HV |
 |
 |
100 |
0 |
0 |
0 |
 |
 |
 |
 |
|
|
 |
|
|
 |
|
 |
|
|
 |
|
| ADDVANCE 6170 |
 |
 |
100 |
0 |
0 |
0 |
 |
 |
 |
 |
|
|
 |
|
|
 |
|
 |
|
|
 |
|
| ADDVANCE 6370 |
 |
 |
100 |
0 |
0 |
0 |
 |
 |
 |
 |
|
|
 |
|
|
 |
|
 |
|
|
 |
|
| ADDVANCE 6380 |
 |
 |
100 |
0 |
0 |
0 |
 |
 |
 |
 |
|
|
 |
|
|
 |
|
 |
|
|
 |
|
| METDRAW 5110 |
 |
|
100 |
0 |
0 |
0 |
|
 |
 |
 |
|
|
 |
|
|
 |
|
 |
|
|
 |
|
| Microlube ML-25 |
 |
|
90 |
0 |
0 |
0 |
 |
 |
 |
 |
|
|
 |
|
|
 |
|
 |
|
|
 |
|
| Microlube ML-450 |
 |
|
90 |
0 |
0 |
0 |
 |
 |
 |
 |
|
|
 |
|
|
 |
|
 |
|
|
 |
|
MPT INDUSTRIES
Dover, NJ
United States
General Purpose Lubricant, Gear Lubricant/Additive, Stamping and Deep Drawing Lubricant
|
| |
|
 |
30-80 |
2-35 |
1-5 |
0 |
 |
 |
|
 |
|
|
|
 |
|
 |
 |
 |
 |
 |
|
 |
PETRON PLUS GLOBAL INC.
Hutchinson, KS
United States
|
| 60050 |
 |
|
100 |
|
|
|
 |
 |
 |
 |
|
|
 |
 |
|
 |
|
 |
 |
 |
 |
|
| 60052 |
 |
|
100 |
|
|
|
 |
 |
 |
 |
|
|
 |
 |
|
 |
|
 |
 |
 |
 |
|
| 60250 |
 |
|
100 |
|
|
|
 |
 |
 |
 |
|
|
 |
 |
|
 |
|
 |
 |
 |
 |
|
| 60610 |
|
 |
100 |
|
|
|
 |
 |
 |
 |
|
|
 |
 |
|
|
|
 |
 |
 |
 |
|
| 55800 |
 |
|
100 |
|
|
|
|
|
 |
 |
|
|
|
 |
|
|
|
 |
 |
|
 |
|
| 55750 |
 |
|
100 |
|
|
|
|
|
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
|
| 55637 |
 |
|
100 |
|
|
|
|
 |
 |
 |
|
|
|
 |
|
|
|
 |
 |
 |
 |
|
| 55630 |
 |
|
100 |
|
|
|
|
|
|
 |
|
|
|
 |
|
|
|
 |
 |
|
 |
|
| 55795 |
 |
|
100 |
|
|
|
|
|
 |
 |
|
|
|
 |
|
|
|
 |
 |
 |
 |
|
PICO CHEMICAL CORP.
Chicago Heights, IL
United States
|
| Picodraw 4030 |
 |
 |
100 |
|
|
|
 |
 |
 |
 |
|
 |
 |
 |
|
 |
|
 |
|
 |
 |
|
| Picodraw 4030 HD |
 |
 |
100 |
|
|
|
 |
 |
 |
 |
|
 |
 |
 |
|
 |
|
 |
|
 |
 |
|
| Picodraw 4042 |
 |
 |
100 |
|
|
|
 |
 |
 |
 |
|
 |
 |
 |
|
 |
|
 |
|
 |
 |
|
| Picodraw 4035 |
 |
 |
94 |
|
|
|
 |
 |
 |
 |
|
 |
 |
 |
|
 |
|
 |
|
 |
 |
|
| Picodraw 4036 |
 |
 |
100 |
|
|
|
 |
 |
 |
 |
|
 |
 |
 |
|
 |
|
 |
|
 |
 |
|
| Picodraw 4039 |
 |
 |
90 |
|
|
|
 |
 |
 |
 |
|
 |
 |
 |
|
 |
|
 |
|
 |
 |
|
| Picolube RL 220 |
 |
 |
100 |
|
|
|
|
 |
 |
 |
|
 |
 |
 |
|
 |
|
 |
|
|
 |
 |
| Picocool 5252 |
 |
 |
98 |
|
|
|
 |
 |
 |
 |
|
 |
 |
 |
|
 |
|
 |
|
 |
|
 |
| Picocut 6071 |
 |
 |
96 |
|
|
|
 |
 |
 |
 |
|
 |
 |
 |
|
 |
|
 |
|
 |
 |
 |
| Picocut 6075 |
 |
 |
100 |
|
|
|
 |
 |
 |
 |
|
 |
 |
 |
|
 |
|
 |
|
|
 |
 |
| Picocut 6076 |
 |
 |
94 |
|
|
|
 |
 |
 |
 |
|
 |
 |
 |
|
 |
|
 |
|
|
 |
 |
| Picocut 6079 |
 |
 |
100 |
|
|
|
 |
 |
 |
 |
|
 |
 |
 |
|
 |
|
 |
|
|
 |
 |
| Picosol 5385 |
 |
 |
100 |
|
|
|
 |
 |
 |
 |
|
 |
 |
 |
|
 |
|
 |
|
|
 |
 |
| Picomist 4098 |
 |
 |
100 |
|
|
|
 |
 |
 |
 |
|
 |
 |
 |
|
 |
|
 |
|
|
 |
 |
| Picolube BCL |
 |
 |
87 |
|
13 |
|
 |
 |
 |
 |
|
 |
 |
 |
|
 |
|
 |
|
|
 |
 |
PPX INC.
Hutchinson, KS
United States
|
| 60060 |
 |
 |
|
|
|
|
|
 |
 |
 |
|
|
 |
 |
|
 |
|
 |
 |
 |
 |
|
| 61612 |
 |
 |
|
|
|
|
|
 |
 |
 |
|
|
 |
 |
|
 |
|
 |
 |
 |
 |
|
| 61614 |
 |
 |
|
|
|
|
|
 |
 |
 |
|
|
 |
 |
|
 |
|
 |
 |
 |
 |
|
| 61620 |
 |
 |
|
|
|
|
|
 |
 |
 |
|
|
 |
 |
|
 |
|
 |
 |
 |
 |
|
| 61630 |
 |
 |
|
|
|
|
|
 |
 |
 |
|
|
 |
 |
|
 |
|
 |
 |
 |
 |
|
| 61622 |
 |
 |
|
|
|
|
|
 |
 |
 |
|
|
 |
 |
|
 |
|
 |
 |
 |
 |
|
| 61638 |
 |
 |
|
|
|
|
|
 |
 |
 |
|
|
 |
 |
|
 |
|
 |
 |
 |
 |
|
| 61640 |
 |
 |
|
|
|
|
|
 |
 |
 |
|
|
 |
 |
|
 |
|
 |
 |
 |
 |
|
| 61644 |
 |
 |
|
|
|
|
|
 |
 |
 |
|
|
 |
 |
|
 |
|
 |
 |
 |
 |
|
| 61646 |
 |
 |
|
|
|
|
|
 |
 |
 |
|
|
 |
 |
|
 |
|
 |
 |
 |
 |
|
SYNTHETIC LUBRICANTS INC.
Greenville, MI
United States
|
| Sawzit |
 |
|
|
0 |
0 |
0 |
|
|
 |
 |
|
|
|
 |
|
|
|
 |
 |
|
 |
|
| Sawzit NF |
 |
|
|
0 |
0 |
0 |
|
|
 |
 |
|
|
|
 |
|
|
|
 |
 |
|
 |
|
| Grindzal |
 |
|
|
0 |
0 |
0 |
|
|
 |
|
|
|
|
 |
|
|
|
 |
 |
 |
 |
|
TOWER OIL & TECHNOLOGY CO.
Chicago, IL
United States
|
| Tower X-44 |
 |
 |
100 |
|
|
|
 |
 |
 |
 |
|
|
 |
|
|
 |
|
 |
|
|
 |
|
| Tower X-65 |
 |
 |
100 |
|
|
|
 |
 |
 |
 |
|
|
 |
|
|
 |
|
 |
 |
 |
 |
|
| Tower X-67 |
 |
 |
100 |
|
|
|
 |
 |
 |
 |
|
|
 |
|
|
 |
|
 |
|
|
 |
|
ULTRALUBE BIOBASED LUBRICANTS
Dixon, IL
|
| Multipurpose Lube & Penetrant, Aerosol (10443, 10444) |
 |
|
>65 |
|
|
|
 |
|
 |
|
|
|
|
 |
|
 |
|
 |
 |
 |
|
 |
| Industrial-grade Rust & Corrosion Inhibitor, Aerosol (10466) |
 |
|
>50 |
|
|
|
 |
|
 |
|
|
 |
|
 |
|
|
|
|
|
|
|
 |
| Multipurpose Lube & Penetrant, Non-aerosol (10445, 10446, 10447, 10448, 10449, 10450) |
 |
|
>95 |
|
|
|
 |
 |
 |
 |
|
|
|
 |
|
 |
|
 |
 |
 |
|
 |
| Industrial-grade Penetrant, Non-aerosol (10460, 10461, 10462) |
 |
|
>90 |
|
|
|
 |
 |
 |
 |
|
|
|
 |
|
|
|
|
|
|
|
 |
| Industrial-grade Penetrant, Aerosol (10463) |
 |
|
>60 |
|
|
|
 |
|
 |
|
|
|
|
 |
|
|
|
|
|
|
|
 |
| Industrial-grade Lubricant, Aerosol (10464) |
 |
|
>65 |
|
|
|
 |
|
 |
|
|
 |
|
 |
|
|
|
|
|
|
|
 |
| Industrial-grade Lubricant, Non-aerosol (10465) |
 |
|
>95 |
|
|
|
 |
|
 |
|
|
|
|
 |
|
 |
|
 |
 |
 |
|
 |
| Industrial Gear Lube, ISO 140 (10592, 10593) |
 |
|
>70 |
|
|
|
|
|
|
 |
|
|
|
 |
|
|
 |
|
|
|
|
 |
| Industrial Gear Lube, ISO 220 (10598, 10599) |
 |
|
>70 |
|
|
|
|
|
|
 |
|
|
|
 |
|
|
 |
|
|
|
|
 |
| Drilling & Tapping Fluid (10664) |
 |
|
>75 |
|
|
|
 |
 |
 |
 |
|
|
|
 |
|
|
|
 |
 |
 |
|
 |
| H1 Food-grade Chain & Cable Lube, Aerosol (10500) |
 |
|
>90 |
|
|
|
 |
|
 |
|
|
|
|
 |
|
 |
|
 |
 |
 |
|
 |
| H1 Food-grade Chain & Cable Lube, Non-aerosol (10505, 10506) |
 |
|
>95 |
|
|
|
 |
 |
 |
 |
|
|
|
 |
|
 |
|
 |
 |
 |
|
 |
| H1 Food-grade Hydraulic Oil, ISO 32/46 (10583) |
 |
|
>95 |
|
|
|
|
|
|
 |
|
|
|
 |
 |
|
|
|
|
|
|
 |
| Hydraulic Oil ISO 32/46/68 (10557, 10560, 10563) |
 |
|
>80 |
|
|
|
|
|
|
 |
|
|
|
 |
 |
|
|
|
|
|
|
 |
| Hydraulic Oil ISO 220 (10594, 10595) |
 |
|
>90 |
|
|
|
|
|
|
 |
|
|
|
 |
 |
|
|
|
|
|
|
 |