thefabricator.com
FFID Search
Advertise with Us
Marketing Services
Add Company
Guide Login
Buyers' Guides
Manual Plasma Arc Cutting Power Source Buyers' Guide©
Model or Series
Input
Output
Current
(Amps)
Duty
Cycle
Capacity (Inches)
Weight
(lbs.)
Arc
Start
Volts
Phase
Hertz
1
3
50
60
ESAB WELDING & CUTTING PRODUCTS
Florence, SC
HandyPlasma® 250
115
120
18
20
.25
.375
.25
20
22
70
4.17
Handy Plasma 380
208/230
120
30
35
.375
.50
10
22
4
PowerCut 650
208/230
120
40
40
.625
.75
8
53
80
PowerCut 900
208/230, 460
120
60
60
.875
1.25
.375
10
71
80
6.6
PowerCut 1300
208/230/460, multivoltage, 575
120
70
100
1.125
1.50
.5
6
90
80
6.6
PowerCut 1600
208/230/460, multivoltage, 575
120
90
60
1.50
1.75
.75
7
90
80
6.6
ESP-150
230/460/575
120
150
90
2.0
2.5
1.0
5
756
100
Deuce Pack
230/460/575
120
300
90
4.0
4.5
1.5
5
1,320
70
HYPERTHERM INC.
Hanover, NH
Powermax30
120 - 230
83
15 - 30
2.49
50
40
.25
.375
.5
20
20
90
3.5
Powermax45
200 - 240
132
20 - 45
50
40
.5
.75
1.0
.375
25
37
90
6
Powermax65
200 - 600
139
20 - 65
50 - 100
40
.75
1.0
1.25
.625
20
64
85
6.7
Powermax85
200-600
143
25 - 85
40 - 100
40
1.0
1.25
1.5
.75
20
71
85
6.7
Powermax1650
200 - 600
160
30 - 100
16
60 - 80
40
1.25
1.5
1.75
.75
19
135
75
9.2
MAX200
220 - 480
150
40 - 200
30
100
40
1.5
2
2.5
1
13
780
120
1.1
C&G SYSTEMS
Libertyville, IL
US
Aviator DSD
240/480
Up to 130
100
1.0
1.5
1.0
21.5
Crossfire
240/480
Up to 400
100
2.0
3.0
2.0
31.5
Taurus
240/480
Up to 1,000
100
2.0
3.0
2.0
31.5
EASYWELD WELDING LOGISTICS CO.
New Territories,,
Hong Kong SAR
EasyCut 40
220
220
5 - 40
4.8
60
60
.4
.49
.49
.49
4
18
58
6.3
FASTENAL
Winona, MN
Blackstone 230
230
230
40
35
.375
.25
.25
.25
.375
21
60
4.5
LINCOLN ELECTRIC CO., THE
Cleveland, OH
Tomahawk™ 375 Air
208/230
90
25
35
.3125
.375
.5
22
40
80
2.1
Tomahawk™ 625
208/230
96
40
35
.5
.625
.75
20
34
80
2.1
MILLER ELECTRIC MFG. CO.
Appleton, WI
Spectrum 875 Auto-Line
208-575
140
60
9.7
60
40
.875
1.25
.437
13
56
90
6.75
Spectrum 875
208/230
140
60
9.8
50
40
.875
1.25
.437
13
56
90
6.75
Spectrum 625 X-TREME
208/230
140
40
6.6
50
40
.625
.875
.312
14
21
90
6
Spectrum 375 X-TREME
115/230
92
27
3.2
35
40
.375
.625
.187
17
18
90
4.5
Spectrum 375
115/230
90
15-27
3.2
35
40
.375
.625
.187
17
55
90
120
Spectrum 125C
120
110
12
2.0
35
40
.125
31
MULTIPLAZ NORTH AMERICA
Santa Monica, CA
Multiplaz 3500
110/230
9.6
2.0/3.5
100
.375
.5625
24
NU-TEC SYSTEMS LLC
Gurnee, IL
Nu-Tec PCA28
115
96
18
1.6
40
40
.1875
.3750
.3125
.1875
25
22
40
3.1
Nu-Tec PCA38
230
94
30
2.8
35
40
.250
.625
.500
.250
25
24
40
3.1
Nu-Tec PCA58
230
98
48
4.5
35
40
.500
1.00
.875
.500
23
27
70
6.1
Nu-Tec PCA28K
115
86
14
1.3
30
40
.125
.250
.1875
.125
26
29
OTC DAIHEN INC.
Tipp City, OH
D12000
230/460
30 - 120
100
2.0
2.5
2.5
2.5
384
60