| Service Name | Count | Percentage of Total |
|---|---|---|
| welding | 31 | 78% |
| machining | 25 | 63% |
| laser cutting | 22 | 55% |
| punching | 19 | 48% |
| assembly | 18 | 45% |
| bending | 16 | 40% |
| powder coating | 16 | 40% |
| forming | 14 | 35% |
| finishing | 10 | 25% |
| painting | 9 | 23% |
| stamping | 9 | 23% |
| drilling | 8 | 20% |
| design | 7 | 18% |
| hardware insertion | 7 | 18% |
| plasma cutting | 6 | 15% |
| rolling | 6 | 15% |
| sawing | 6 | 15% |
| silk screening | 6 | 15% |
| waterjet cutting | 6 | 15% |
| engineering | 5 | 13% |
| shearing | 5 | 13% |
| tube bending | 5 | 13% |
| cutting | 4 | 10% |
| fabricating | 4 | 10% |
| flame cutting | 3 | 8% |
| plating | 3 | 8% |
| structural steel fabricating | 3 | 8% |
| grinding | 2 | 5% |
| heat treating | 2 | 5% |
| inventory management | 2 | 5% |
| logistical services | 2 | 5% |
| packaging | 2 | 5% |
| plate fabricating | 2 | 5% |
| prototyping | 2 | 5% |
| roll bending | 2 | 5% |
| structural steel bending | 2 | 5% |
| tapping | 2 | 5% |
| tooling production | 2 | 5% |
| edm | 2 | 5% |
| airflow inspection | 1 | 3% |
| brazing | 1 | 3% |
| contact manufacturing | 1 | 3% |
| detailing | 1 | 3% |
| e-coating | 1 | 3% |
| electrical | 1 | 3% |
| etching | 1 | 3% |
| graphics printing | 1 | 3% |
| guage calibration | 1 | 3% |
| laser tube cutting | 1 | 3% |
| laster cutting | 1 | 3% |
| nondestructive testing | 1 | 3% |
| notching | 1 | 3% |
| oxidized edge removal | 1 | 3% |
| oxyfuel cutting | 1 | 3% |
| phosphatizing | 1 | 3% |
| presicion grinding | 1 | 3% |
| roll forming | 1 | 3% |
| tool and die production | 1 | 3% |
| toolding production | 1 | 3% |
| tube cutting | 1 | 3% |
| turning | 1 | 3% |
| warehousing | 1 | 3% |
| woodworking | 1 | 3% |