Mechanical Press Buyers' Guide©

Model Capacity Range
(tons)
Clutch/
Brake
Gearing
Arrangement
Suspension
Points
Stroke
Length
(min. - max.,
inches)
Shut Height Over Bed Slide Down Adjustment Up  with standard stroke min max inches Maximum SPM Guiding Structure
4 Point 6 Point 8 Point Gap or C Frame Inclinable Straight side with Tie Rod Straight side without Tie Rod Knuckle Joint
Pneumatic Hydraulic Servo Flywheel nongear Single Gear Double Gear Link Other Single Multiple

 Hot Link - Amada America, Inc. - MechanicalPress AMADA AMERICA, INC. Buena Park, CA United States   Email Icon - Amada America, Inc. - MechanicalPress Video Icon - Amada America, Inc. - MechanicalPress

TP-EX Series
49.5 - 275
             
2 - 12
9 - 21.6
100
           
TPL Series
49.5 - 330
           
2 - 12
9 - 18
125
         
TPW Series
121 - 330
             
3 - 12
10 - 20
125
           
TPWL Series
110 - 550
           
3 - 12
10 - 20
125
         
SDE Series
49.5 - 330
             
0 - 12
11.4 - 21.6
225
         
SDEW Series
220 - 330
             
3- 10
10 - 17, 12- 19
60, 80
           

 Hot Link - Komatsu America -  Press Technology Div. - MechanicalPress KOMATSU AMERICA - PRESS TECHNOLOGY DIV. Rolling Meadows, IL United States  

H2F Series Straight Side Servo
220 - 2,500
         
0 - 15.7
20.5-37.4
80
         
OBS Series General Purpose
29 - 220
             
2 - 11.8
7.7-18.9
240
           
W Series General Purpose
121 - 330
             
4.3 - 11.8
14.7-21.6
100
         
G Series General Purpose
220 - 4,500
         
3.9 - 32.6
20.1 - 37.4
150
           
M Series Progressive Die
220 - 3,000
         
3.9 - 11.8
18.7 - 27.5
150
           
S Series Auto Class Transfer
1,000-5,000
         
18.9-43.5
25.6-65.5
30
           
B Series Heavy Blanking
220-550
           
3.9-11.8
17.8-25.6
100
           
C Series Forging
176-2,200
         
3.5-15.8
13.4-55.1
75
         
H1F Series Gap Frame Servo Press
29 - 220
             
0 - 9.8
8.2-17.7
230
       
H2W Series Solid Frame Servo
220 - 330
             
5.9 - 13.8
19.7 - 23.6
85
           

 AIDA-AMERICA Dayton, OH United States

NC1 Series
35 - 250
           
3 - 12
9.8 - 17.7
130
           
NC2 Series
110 - 250
           
4.3 - 11
13.7 - 21.6
100
           
PMX Series
300 - 1,000
             
6 - 16
24 - 40
90
             
SMX Series
300 - 2,000
           
To spec.
24 - 40
30
           
TMX Series
300 - 4,000
           
To spec.
24 - 40
30
           
HMX Series
80 - 400
             
.8 - 3
 
800
             
NSU Series
200-400
                 
8-12
 
100- 65
           
NST Series
300 - 1,200
         
10 - 24
To spec.
60 - 40
           
NS1 Series
80 - 200
             
3 - 10
9.8 - 17.7
130
             
NS2 Series
110-300
             
4.3-11
13.7-21.6
100- 35
             
MCX
315-1,250
                               

 DANLY AND VERSON BY ENPROTECH Lansing, MI United States

 
25 - 3,500
                   

 EAGLE PRESS & EQUIPMENT CO. LTD. Oldcastle, ON Canada

SC2
100 - 1,000
     
2 - 20
To spec.
80
         
SE2
400 - 2,000
       
8 - 30
To spec.
60
           
SE4
600 - 3,500
       
8 - 32
To spec.
60
           

 FAGOR ARRASATE USA INC. Willowbrook, IL United States

Blanking
440 - 1,500
       
8 - 18
48 - 60
80
           
Double Action
1,100 - 3,200
         
40 - 60
60 - 78
25
           
General Purpose
400 - 4,000
       
30 - 60
18 - 70
50
           
Monoblock
100 - 800
       
4 - 24
24 - 40
150
           
Progressive Die
300 - 2,500
       
16 - 24
36 - 50
60
           
Tandem Line
400 - 8,500
     
28 - 60
50 - 78
25
         
Transfer
250 - 5,700
     
24 - 50
36 - 78
45
         
Tryout
1,100 - 4,000
           
40 - 80
60 - 78
20
           
Forging
500 - 1,500
         
16 - 24
40 - 50
50
           
Servo Presses
300-2,500
           
Var.
Var.
Var.
           

 FOREMOST MACHINERY CORP. Northbrook, IL United States

3A RMT
3
                 
0-2
6
240
             
5B RMT
6
                 
0-2
7
240
             
7B RMT
8
                 
0-1.312
7.687
240
             
6C RMT
8
                 
0-3.125
6.75
240
             
8C RMT
9
                 
0-2.50
7.50
240
             
10C RMT
10
                 
0-2
8
240
             
12C RMT
12
                 
0-1.50
8.50
240
             
18D RMT
18
                 
0-2.50
8.50
120
             
20D RMT
20
                 
0-2
9
120
             
24D RMT
24
                 
0-1.50
9.50
120
             

 HEIM GROUP, THE Chicago, IL United States

Single Point Gap Frame
15-300
           
1-14
6.75-32
180
       
Two Point Gap Frame
40-300
         
1-12
1.75-26
120
       
Single Point Straight Side
90-300
           
2-10
12-20
115
             
Two Point Straight Side
40-400
           
1-12
5-28.25
115
           
S2 Series Maxi-Stamper Straight Side
200-1,000
           
6-12
20-42
80
           
H2 Series Maxi-Stamper Straight Side
100-300
           
1-4
13.5-23
200
           
S1 Series Maxi-Stamper II
90-300
         
2-10
12-20
150
           

 MINSTER MACHINE CO., THE Minster, OH United States

P2H-FX
100-160
             
2.95-7.87
11.00-23.62
250
         
FX2
600
             
15.75-19.69
24-44
70
           
MMC Series Gap
45-315
         
1.97-11.02
9.84-21.65
150
           
HB Series
66 - 90
             
.59 - 2.5
13 - 19.0
1,000
             
P2 Series
60 - 200
           
1 - 8
11 - 20
600
           
P2H Series
71 - 180
           
.79 - 7.88
8.9 - 23.6
600
           
PM3 Series
125 - 300
             
1.0 - 2.5
15 - 17
800
           
PM4 Series
250 - 600
             
1.18 - 1.57
To spec.
535
           
E2 Series
200 - 1,600
         
4 - 24
19 - 50
150
           
E2H/E2HF Series
250 - 600
       
1.18 - 15.75
To spec.
375
           
E4H Series
880 - 2,200
         
11.81 - 29.53
26.75 - 75.67
80
           
NTCH
10-25
             
.472
7.067 - 8.067
1,200
             
MMC Series S.S.
160-1,200
             
5.12-31.50
15.75-51.18
85
           
Minster Kyori ANEX
15-125
             
.39-1.97
8.66-13.78
1,800
           
Minster Kyori VX
40-80
             
.63-1.97
9.45-12.60
1,000
           

 OAK PRESS SOLUTIONS INC. Sturgis, MI United States

LP Series
30-300
             
1.00-3.00
 
400
           
SS Series
30-60
             
.50-2.00
 
1,500
           
P1 Series
30-45
             
1.00-2.00
 
1,000
           
CP Series
120-160
             
1.00-3.00
 
400
           

 PRESS AUTOMATION INC. Elkhart, IN United States

         

 SANGIACOMO PRESSE Vittorio Veneto, Italy

C-Frame Flywheel Presses
10-75
             
.24-5.51 adjustable
6.7-12.21
230
         
C-Frame Back Geared Presses
50-450
             
.47-9.84 adjustable
11.42-23.62
100
         
Straight-side Presses Single Connecting Rod
50-250
           
.47- 9.06 adjustable
11.81-21.65
200
           
Straight-side Presses Double Connecting Rod
125-500
           
.55-15.75 adjustable
17.72 - 27.56
90
           

 SCHULER INC. Canton, MI United States

SPE S Series Prog. Die
1,100 - 1,750
             
20 - 24
48 - 52
50
           
STL4 S Series Transfer
1,350 - 3,500
             
24 - 36
50 - 60
30
           
PME2 and PME4 Progressive Die
880 - 3,600
             
16
39.4 - 55.1
60
           
PML2 and PML4 Prog. Die
880 - 3,600
             
20
39.4 - 55.1
50
           
TME2 and TML2 Transfer
880 - 3,600
           
20 - 36
47.2 - 55.1
40
           
TML4 Transfer
To spec.
             
To spec.
To spec.
To spec.
           
MSD Servo Drive
280-900
             
2.4-16
24-39
130
           
TMK Transfer & Progressive Die
220 - 1,100
           
1.5 - 10
15 - 30
140
         
SAK High-Speed Blanking
175-275
             
1 - 2
15-17
800
           
SML4 Car Body
880 - 2,800
             
36 - 43.3
To spec
20
           
SAL High-Speed Lamination
137 - 550
             
1.2 - 1.4
16 - 23
1,000
           
XS Impact Extrusion
165 - 1,350
           
13 - 23
 
300
           
MSK Servo Knuckle Joint
280-1,100
             
6-12
23-31
160
       
TSD/TSC Servo Drive
900 - 3,375
             
6 - 30
39 - 55
50
           

 SEYI-PRESSES INC. Tullahoma, TN United States

SN1 Gap
28 - 275
           
1.38 - 9.84
7.87 - 17.72
180
           
SN2 Gap
121 - 330
           
2.75 - 11.02
13.78 - 21.65
120
           
SNS1 Straight Side
88-330
         
2.36-11.02
11.81-19.69
150
         
SLS1 Link Motion Straight Side
88 - 330
         
3.94 - 9.84
11.81 - 17.72
110
           
SNS2 Straight Side
176-440
       
3.15-11.81
15.75-23.62
115
         
SLS2 Link Motion Straight Side
176 - 440
         
5.12 - 11.81
15.75 - 23.62
90
           
SAG Straight Side
330-1,300
       
To spec.
To spec.
To spec.
         
SLG Link Motion Straight Side
330 - 1,300
       
To spec.
To spec.
To spec.
         
SM2 High Speed Link Motion Straight Side
220 - 660
         
7.87 - 9.84
17.72 - 29.52
120
           
SM1 Heavy Stamping Link Motion Straight Side
330 - 880
         
4.72 - 11.81
15.75 - 29.50
70
           
SE Eccentric Gear Straight Side
440-2,400
       
To spec.
To spec.
To spec.
           
SEL Link Motion Eccentric Gear Straight Side
440 - 2,400
       
To spec.
To spec.
To spec.
           
SPF2 Progressive Cold Forging Straight Side
220 - 440
         
4.72
17.72 - 19.68
100
         
SH1 High Speed Straight Side
22 - 50
             
1.18 - 1.57
7.87 - 9.65
700
           
SH2 High Speed Straight Side
50 - 66
           
1.18 - 1.96
9.25 - 12.20
700
           

 STAMTEC INC. Manchester, TN United States

OCP Single Point Gap Frame Presses
25 - 260
           
1.57 - 11.81
9.65 - 21.26
180
           
G2 Series Two Point Gap Frame Presses
110 - 250
           
4.33 - 11.02
15.75 - 21.65
100
           
GL1 Link Motion Single Point Gap Frame Presses
80 - 200
         
3.94 - 7.87
11.8 - 17.7
110
           
GL2 Link Motion Two Point Gap Frame Presses
110 - 260
         
4.33 - 11.02
15.8 - 21.7
90
           
SC1 Single Point Straight Side Presses
160 - 287
           
3.15 - 7.87
13.78 - 18.11
115
           
SC2 Two Point Straight Side Presses
121 - 275
           
3.15 - 7.87
13.78 - 18.11
115
           
S1 Single Point Straight Side Presses
165 - 660
       
5.91 - 12.2
15.75 - 30.12
120
           
GTX Two Point Straight Side Presses
160 - 440
           
5.12 - 11.81
17.72 - 21.65
85
           
S2 Two Point Straight Side Presses
165 - 660
       
5.91 - 12.2
15.75 - 30.12
120
         
SLX Link Motion Two Point Straight Side Presses
160 - 300
         
3.94 - 5.91
17.72
100
           
HSD High-speed Straight Side Presses
60 - 300
             
1.18
13 - 17
550
           
4-Point Straight Side
To 3,000
           
To spec.
To spec.
To spec.
           
Transfer Presses
To 3,000
           
To spec.
To spec.
To spec.
           
KP, KT, KL, KW2 Series Forging Presses
250 - 2,000
           
To spec.
To spec.
To spec.
           
F2 Series Warm-Hot Forging Presses
700 - 3,000
           
To spec.
To spec.
To spec.