Stamping Lubricant Buyers' Guide©

Series/Formula
Name
Operation Chemistry Application Method Metal Cleaning
Method
Hazardous
Materials
Identification
Systems (HMIS)
Deep Drawing Light Medium Stamping Drawing Heavy Stamping Drawing Severe Stamping Drawing Dry Film Water Soluble Oil Straight Oil Semisynthetic Synthetic Solvent Precoat Dry Film Precoat Wet Film Roller Coating Manual Hand Drip Flood Airless Spray Aluminum Aluminized Brass Copper Stainless Steel Steel Galvanized Galvannealed Aqueous Solvent Health Hazard Flammability Reactivity Personal Protection

 CHEMTOOL INC. Crystal Lake, IL United States

ReNu 920                 1 1 0 B
ReNu 900 WS                 1 1 0 B
NuSol Lubriform Penultimate                     1 1 0 B
Nusol Lubriform Superior                     1 1 0 B
CT 499                         1 1 0 B
Lubridraw 3305 WX                       1 1 0 B
Lubridraw 3320               1 1 0 B
Lubridraw 3495                     1 1 0 B
Lubridraw 3490                   1 1 0 B
CT 3302                 1 1 0 B
CT 3304             1 1 0 B
Lubriform 3900                     1 1 0 B
Lubriform 3905               1 1 0 B
Lubriform 3935                     1 1 0 B
Lubriform 4200                     1 1 0 B
Lubriform 500 CF                     1 1 0 B
Lubriroll 4240                               1 1 0 B
CT 3340                   1 1 0 B
CT 3388 CU                       1 1 0 B
CT 3425                         1 1 0 B

 ETNA PRODUCTS INC. Chagrin Falls, OH United States

Masterdraw 6050B                       1 1 0 C
Masterdraw 727                     1 1 0 C
Masterdraw 7002HVRP                         1 0 0 C
Masterdraw VOL G                         1 3 0 C
Daphne AF2AU                         1 3 0 C
Daphne AF8AU                         1 1 0 C
Masterdraw SOL G                       1 1 0 C
Masterdraw SOL H 3850                         1 1 0 C
Masterdraw SOL S 3950                     1 1 0 C
Masterdraw SSY G-4100                           1 1 0 C
Masterdraw SSY G-4200                         1 1 0 C
Masterdraw SSY H                         1 1 0 C
Masterdraw SSY S                 1 0 0 C
Masterdraw SYN G                       1 1 0 C
Masterdraw SYN H                         1 1 0 C
Masterdraw SYN S-5100                       1 1 0 C
Masterdraw SYN S-5200                       1 1 0 C
Masterdraw SP 434                             1 0 0 C
Masterdraw SP 417                             1 0 0 C

 FUCHS LUBRICANTS CO. Harvey, IL United States

Eco Draw HVE-1                       1 0 0 A
Eco Draw HVRG-8                       1 0 0 A
Eco Draw HVE-2                       1 0 0 A
Eco Draw 7905                           1 0 0 A
Renoform OS 7910                           1 0 0 A
Montgomery DB 4265 C               1 0 0 B
Montgomery DB 4265 BW                   1 0 0 B
Tuf Draw 2806 M-100                     1 1 0 B
Tuf Draw HPAL                 1 1 0 B
Anticorit PL 3802-39 LV8 US                 1 1 0 B
Anticorit PL 3802-39S                               1 1 0 B
Anticorit 4107-S                                   1 1 0 B
Renoform FB 2000                               1 1 0 B
Renoform FB 43 Light                               1 1 0 B
Renoform EXT 319 IS                             1 0 0 B
Renoform EXT 519                             1 1 0 B
Anticorit PL 39 SX                             1 1 0 B

 IRMCO LEANGREEN METALFORMING Evanston, IL United States

080-00B                         1 0 0  
136-000                             1 0 0  
125-00M                               1 0 0  
090-100                               1 0 0  
146-000                             1 0 0  
156-00I                             1 0 0  
313-00A                               1 0 0  
323-M80                             1 0 0  
536-37Z                             1 0 0  
136-292                             1 0 0  
146-292                             1 0 0  
536-00U                             1 0 0  
323-00M                             1 0 0  
136-492                                   1 0 0  
156-495                                 1 0 0  
146-892                           1 0 0  

 JOHN NEALE LTD. Halesowen, United Kingdom

Superdraw FS                           1 0 0 A
Superdraw ST2000                       1 0 0 A
Coating Lubricant CR                                       1 1 0 A
Vanishing Oil JN60                           1 1 0 A
Superdraw SG                   0 0 0 A
Tube Lubricant JN7+                             1 0 0 A
Tube Bending Resin WS8                               1 0 0 A

 LAMSON OIL CO. Rockford, IL United States

HeavyDraw 1100 Series                      
HeavyDraw 1200 Series                      
FormAll 2200 Series                          
FormAll 2300 Series                        
LamSyn 3000 Series                              
LamSyn 4200 Series                                  
Vanish 6800 Series                                
Vanish 6900 Series                              

 MPT INDUSTRIES Dover, NJ United States

MPT Industrial Lubricant                         1 1 0 A

 PETRON PLUS GLOBAL INC. Hutchinson, KS United States

Compound 55660                 1 1 0  
Compound 55665                 1 1 0  
Compound 55671               1 1 0  
Compound 55643                   1 1 0  
Metalform 2000 52190               1 1 0  
Metalform 2000-HD 57140             1 1 0  
Metalform 2000-P 52195               1 1 0  
Metalform 3000-P 55611               1 1 0  
Metalform 4000-P               1 1 0  
Metalform 6000 52232               1 1 0  
Metalform 7000 52215               1 1 0  

 PICO CHEMICAL CORP. Chicago Heights, IL United States

Picodraw 4067                         1 1 0  
Picodraw 4066                             1 1 0  
Picodraw 4030                     1 0 0  
Picodraw 4042                   1 0 0  
Picodraw 4030 Gel                               1 0 0  
Picodraw 4036                   1 0 0  
Picodraw 4015                       1 0 0  
Picosol 5381                   1 1 0  
Picocut 6012                         1 1 0  
Picoform 4700                                   1 2 0  
Picoform 4730                                       1 2 0  
Pico Extrud 412P                     1 1 0  
Picomist 4098                     1 1 0  

 PPX INC. Hutchinson, KS United States

Metalpro Alpha – 52199                   1 1 0  
Metalpro Beta – 52204                   1 1 0  
Metalform 2000 – 52190                   1 1 0  
Metalform 2000-P – 52194                   1 1 0  
Metalform 2000-HD – 57140                   1 1 0  
Synthetic Drawing & Stamping Compound – 55661                   1 1 0  
Heavy-Duty Synthetic Drawing & Stamping Compound – 55666                   1 1 0  
Industrial Super Lube – 12845                   1 1 0  
Light-Duty Straight Oil – 55760                   1 1 0  
Med-Duty Straight Oil – 55762                     1 1 0  
H-D– Straight Oil – 55782                   1 1 0  
Extra H-D Straight Oil – 58590                   1 1 0  
General-Purpose Soluble Oil – 55764                   1 1 0  
H-D G-P Soluble Oil – 55766                   1 1 0  
H-D G-P Soluble Oil w/Chlorine – 55835                   1 1 0  
Semi-Synthetic G-P Soluble Oil Med.-Heavy-Duty                 1 1 0  
Enviro Extra H-D G-P Lubricant – 55732                   1 1 0  
Enviro Mist Lubricant – 55745                   1 1 0  
Synthetic G-P Machining Fluid – 55768                   1 1 0  
H-D Synthetic G-P Machining Fluid – 55786                   1 1 0  

 SOLVITE CHEMICAL CO. Aurora, OH United States

Prodraw 100                         1 1 0 B
Prodraw 125                           1 1 0 B
Prodraw 150                             1 1 0 B
Prodraw 175                           1 1 0 B

 TOWER OIL & TECHNOLOGY CO. Chicago, IL United States

TowerDraw A-406                       1 2 0 B
Saf-T-Vanish GREEN 25                           0 0 0 A
Saf-T-Vanish 125                         0 0 0 A
Saf-T-Draw 100                   0 0 0 A
TowerPro 7800                       1 1 0 B
Towersol G-9196                     1 1 0 B
Hybridraw 8600                 1 0 0 B
Tower 6523-CF                             1 1 0 B
TowerDraw 9890                         1 1 0 B
KleneDraw W-4701                   1 0 0 A
Tower CF-1301                           1 1 0 B
TowerDraw AA-604                           1 2 0 B
KleneDraw 3421                   1 0 0 A
Saf-T-Cool 458                       1 0 0 B
Lamstamp 3488                   1 0 0 A
TowerDraw 9833                     1 1 0 B
TowerPro 7725-E                 1 1 0 B
KleneDraw W-4801                     1 0 0 B

 WALLOVER OIL CO. Strongsville, OH United States

Vanishing Oil 3                         1 2 0 B
Prodraw 365                       1 0 0 B
FB Fineblanking Oil                                 1 0 0 B
Wocodraw 19                             1 1 0 B
Wocodraw 34                           2 1 0 B
Prodraw 200                     1 1 0 B
Prodraw 210                                 1 1 0 B
Prodraw 220                     1 1 0 B
Posidraw 300                             1 1 0 B
Posidraw 309                             1 1 0 C
SDC/SDC-H                       2 1 0 B
Woco CHL-20                       2 1 0 B
Prodraw 175                             1 1 0 B
Prodraw 177                             1 1 0 B
Prodraw 100                           1 1 0 B
Prodraw 125                           1 1 0 B
Prodraw 150                               1 1 0 B
Prodraw 178                         1 1 0 B
Prodraw 370                           1 0 0 B