Cascadia Metals Ltd., Delta, B.C., has purchased a cut-to-length line from Herr-Voss Stamco, to be installed at Cascadia's Brandon, Manitoba, facility.

The line will include a Herr-Voss Stamco Precision LevelerĀ®, which will process material from 0.024 to 0.135 in. thick. It also will include a precision EDT roll feed system coupled with a high-speed shear.