Scott Stainless Steel moves to larger facility

January 19, 2012

Scott Stainless Steel Inc. has moved to a facility in Northbrook, Ill., doubling its space and providing room for expansion.

The company distributes flat-rolled stainless steel, coil, and sheet. It stocks Types 304, 304L, 316L, 430, 409, and 201 in all standard finishes in thicknesses from 10 to 28 ga. Coil is available in any slit width between 0.25 and 60 in., and any coil can be leveled to any standard or nonstandard length.