Arnold Magnetic Technologies launches new division name

June 18, 2014

Magnet manufacturer Arnold Magnetic Technologies, Chicago, has announced the rebranding of its Rolled Products division. The division’s new name, Precision Thin Metals (PTM), better reflects the strategic role its thin and ultrathin specialty alloys play in high-efficiency motors, generators, and batteries.

The company offers thin and ultrathin silicon steels and ultrathin nickel, aluminum, and copper alloys for applications in the aerospace, industrial, and energy-storage industries.