Rolled Alloys expands processing capabilities


June 9, 2014

Rolled Alloys, a supplier of stainless steels, nickel, cobalt, and titanium alloys, has expanded the processing capabilities at its 80,000-sq.-ft. service center in Houston. The addition of a new Behringer HBM-540 complements the existing bar saws, a new racking system, and expanded inventory and grades.

The new saw handles 21-in.-dia. bar with a tolerance of +0.125 to 0 in. The facility offers waterjet, shear, and plasma cutting as well.