MG Systems & Welding, Inc. headquartered in Menomonee Falls, Wis., a manufacturer of thermal machining centers, mainly plasma and oxyfuel, has officially changed its name to Messer Cutting Systems, Inc. The decision was made on a corporate level to improve brand consistency among all facilities; Menomonee Falls, Germany, China, India, and Brazil have all made the change.

In 2009 Messer will celebrate 111 years of manufacturing excellence.