American Roll Form Products opens facility in Nevada

February 19, 2013

American Roll Form Products (ARFP), Painesville, Ohio, a manufacturer of custom roll formed products, has opened a 40,000-sq.-ft. satellite facility in North Las Vegas, Nev., to support customers and projects in the Southwest. It will be operational by the end of March 2013, with two rolling mills initially and a third mill installed by the end of June.

The company now has three facilities with a total of 200,000 sq. ft. and 31 rolling mills. Capabilities include prepunching up to 250 tons, turnkey fabrication and assembly, and robotic welding.