Ohio Laser wins SBA award to expand laser tube cutting services

October 10, 2012

Ohio Laser, Columbus, Ohio, has won the annual Ohio Statewide Development Corp. (OSDC) SBA 504 2012 Loan Project of the Year. Ohio Laser, an ISO 9001:2008-certified metal fabricator, provides precision laser cutting services, laser tube cutting, copper cutting, brass cutting, and other metal fabrication services. OSDC selected Ohio Laser from more than 200 companies in their portfolio.

The company used the loan to expand its laser tube and pipe cutting services. The company cuts tube with ODs from 0.6 to 8 in. square and 10 in. round in lengths to 30 ft., wall thicknesses to 0.5 in., and maximum weight of 500 lbs.