The American Society of Mechanical Engineers (ASME), under Section VIII, Division 1, has awarded U and R Stamp certification to Millerbernd Mfg. Co., Winsted, Minn. This accreditation signifies that the company has met the standards of the ASME Pressure Vessel Code and permits the company to manufacture component parts for use in many types of process equipment and HVAC applications that require ASME certification.

Millerbernd Mfg. Co. manufactures rings and cylinders from carbon steel, stainless steel, and aluminum. Rings are fabricated with diameters from 6 to 144 in. and wall thicknesses from 0.5 to 5 in. Cylinders are manufactured with diameters of 7 to 144 in., wall thicknesses from 0.25 to 5 in., and lengths up to 96 in. In-house services include blast finishing, tapping, drilling, and custom machining.