December 14, 2011
Fischer Technology Inc., Windsor, Conn., has opened an additional sales and service office in San Mateo, Calif. The office supports the company's line of coating thickness, material testing, material analysis, and microhardness instrumentation.
The new location provides services including on-site recertification of hand-held coating thickness gauges and benchtop X-ray fluorescence instruments, as well as repairs and preventive maintenance.