September 24, 2012
E. H. Wachs and Orbitalum Tools GmbH (Illinois Tool Works (ITW) companies) have joined forces and will now be identified as the ITW Orbital Cutting & Welding group, offering the same weld preparation equipment, orbital welding systems, and services as in the past.
In addition, customers now can purchase, lease, and order parts, tooling, and accessories under one roof.