Our Sites

Superior Tube earns AS9100 certification

Superior Tube, Collegeville, Pa., has announced its certification to AS9100.

The company is a manufacturer of precision tubing for the aerospace industry, including seamless and welded tubes, straight lengths, and coils in stainless steel, nickel, titanium, and zirconium.