Gas shielded, flux-cored wires suitable for mild steel welding

April 11, 2006

UltraCore™ 712C and 712A80 gas shielded, flux-cored wires from The Lincoln Electric Co. are suitable for mild steel welding applications.

The 712C for tank and shipbuilding applications uses straight CO2. It is versatile and exhibits high impact values regardless of the notch location in the weld joint. Tensiles are capped at 90 KSI for good crack resistance.

The 712A80 for offshore, tank, and pressure vessel fabrication provides superior arc characteristics and high impacts regardless of the notch location in the joint.