September 8, 2011

Thermadyne® Industries' Victor® brand offers newly configured Journeyman® Select outfits that come standard with ESS4 Edge series regulators and environmentally friendly packaging.
In addition to the regulators, the outfits also include the 2460 cutting attachment and the 315 FC torch handle with built-in flashback arresters and reverse-flow check valves. The cutting attachments are available with 75- or 90-degree head angle.
The heavy-duty outfits cut material up to 8 in. and weld material up to 3 in. with the appropriate accessories.
An internal vent system protects the regulator internals from weather elements. Proprietary Shock Limitation and Absorption Mechanism (SLAM) technology, built into the knob, protects regulator vitals and the cylinder valve itself by absorbing more than 5,000 lb.-force of impact energy.