Metal clinching process helps make quick, clean joints in most ductile materials

June 20, 2011

Metal clinching process helps make quick, clean joints in most ductile materials - TheFabricator.com

The MultiLoc® metal clinching process helps make quick, clean joints in most ductile materials. Powered by a Multicyl® air/oil intensifier, the fast-advance stroke is followed by a smooth hydraulic action.

There are several machine alternatives for fastening sheet metal components. Using standard clinching tools in throat depths up to 8 in., the machines can join many combinations of materials, including mild steel; galvanized, prepainted, or precoated stock; aluminum; and stainless steel.