Deep-draw press handles large, deep parts - TheFabricator.com

The model 32-10-12SC deep-draw press from Triform Sheet Hydroforming offers precision forming of a variety of sheet metal parts not suited to traditional forming methods. The 10,000-PSI press features a 32-in.-dia. work area and a 13-in. maximum draw depth capacity.

The press forms complex geometric shapes in a single operation. It eliminates the need for mating dies, and uniform pressure on the metal reduces material thinning. The fully programmable touchscreen controls keep tight control of the pressure and punch position throughout the forming cycle.