Electrodes gouge metals chemical processes cannot


August 8, 2006

Carbon arc electrodes from Weldmark physically remove metal, do not need oxidation to maintain the cut, and gouge metals that chemical processes cannot.

The electrodes can cut carbon steel, stainless steel, many copper alloys, and cast irons.