Thermacut's Silver-Pro electrodes combine a copper electrode body and a solid silver insert. The insert helps improve the conductivity of electricity and dissipates the heat of the plasma arc efficiently to help extend electrode life, the manufacturer reports.

The electrodes are available for the Hypertherm® HPR 130®/260® systems, the ESAB® PT-600® system, and the Kjellberg® PERCUT 160®/170®/370.1® systems.