July 19, 2012

Metabo Corp. offers the Combinator combined cutting and grinding wheel. It eliminates the need to change abrasive wheels during cutting and grinding applications.
The wheel is suitable for cutting, deburring, and light grinding. With three layers of fiberglass measuring 0.078 in. thick, it cuts stainless steel, steel, alloy steel, hardened steel, pipe, tube, and solids.
Available in 4.5-, 5-, and 6-in. Type 27 versions, the wheel employs an improved abrasive/resin formulation for fast cutting with increased wheel life, as well as strength and rigidity for grinding and metal removal applications, the manufacturer reports.