CGW-Camel Grinding Wheels has expanded its line of abrasive wheels with the introduction of its three-in-one combo wheels, which allow for cutting, grinding, and finishing with one wheel, eliminating frequent wheel changes.
When the user tilts the right-angle grinder to a 90-degree position, the wheel cuts; when positioned at a 30-degree angle, it grinds; when used at a 15-degree angle, the wheel finishes.
Manufactured with three complete layers of fiberglass and a white aluminum oxide grain, the 0.094-in.-thick wheels grind stainless steel and steel. A fiberglass net reinforcement helps add strength and flexibility to promote safer cutting, grinding, and finishing. The wheels contain less than 0.1 percent of iron, sulfur, or chlorine for rust-free and corrosion-free results.
The wheels are available in a Type 27 shape, 36 grit size, S-grade, and in 4.5-, 5-, and 6-in. diameters with 7/8 or 5/8-11 arbor holes.