A line of small, thin-profile, Type 1 abrasive wheels for deburring slots, gears, stampings, and castings and cleaning pipe threads is available from Rex-Cut Products Inc.

The wheels feature multiple layers of cotton fiber that are impregnated with aluminum oxide or silicon carbide abrasives and laminated, pressed, and bonded into dense wheels. Continuously exposing fresh abrasives as they work, the wheels come in 1- to 4-in.-dia. sizes from 0.03 to 0.5 in. thick.

The wheels are available in coarse, medium, fine, and very-fine grits with soft or hard bonds.